| 双辊薄带连铸熔池液面波动物理模拟 |
| 文光华 祝明妹 |
| 重庆大学材料科学与工程学院; 重庆 400044 |
|
引用本文:
文光华; 祝明妹 . 双辊薄带连铸熔池液面波动物理模拟[J]. 金属学报, 2000, 36(9): 1001-1004 .
[1] Miyake S. ISIJ International, 1991; 7: 689 [2] Macci F. Steel Times,1995; 6: 230 [3] Legrand H, Martel D. Steel Times, 1998; 3: 104 [4] Bouchard D, Busque F, Hamel F G. Steelmaking ConfProc,Chicago: ISS, 1999; 82: 723r |
|