| 纯银等离子体基离子注入Al层的成分及相分析 |
| 于伟东 夏立芳 |
| 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001 |
|
引用本文:
于伟东; 夏立芳 . 纯银等离子体基离子注入Al层的成分及相分析[J]. 金属学报, 2000, 36(8): 805-808 .
[1] Liu B X. Vacuum, 1991; 1/2: 75 [2] Clapham L, Whition J L. J Appl Phys, 1992; 1: 4014 [3] Antlers A. Surf Coat Technol, 1997; 93: 158 [4] Brown I G, Antlers A, Antlers S, Antlers S, Dickinson MR, MacGill R A. J Vac Sci Techol, 1994; B12(2): 823 [5] Xia Z, Chan C, Meassick S, Purser R. J Vac Set Techol,1995; B13(5): 1999 [6] Ryabchikov A 1. Surf Coat Technol, 1997; 96: 9 [7] Tolopa A. Surf Coat Technol, 1997; 93: 168 [8] Yu W D, Xia L F, Sun Y. Surf Coat Technol, 2000 (inpress) [9] Ji H B, Xia L F, Ma X X, Sun Y, Sun M R. Wear, 1999;225-229: 835 [10] Moulder J F, Stickle W F, Sobol P E, Bomben K D. Handbook of X-Ray Photoelectron Spectroscopy. Minnesota:Perkin-Elmer Corporation Physical Electronics Division,1992: 27 [11] He C X, Zhou Y H, Wang W N. Phase Diagrams of Precious Metal Alloys First Supplement. Beijing: Metallurgical Iindustry Press, 1993: 1(何纯孝,周月华,王文娜.贵金属合金相图第一补编北京:冶金工业出版社, 1993: 1)M |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|