| 主族金属元素电子脱出功的计算 |
| 王贵昌 赵玉藏 |
| 南开大学化学系; 天津 300071 |
|
引用本文:
王贵昌; 赵玉藏 . 主族金属元素电子脱出功的计算[J]. 金属学报, 2000, 36(8): 790-792 .
[1] Wen Y K, Shao J. The Theory of Ionic Polarization.Hefei: Anhui Education Press, 1985: 197(温元凯,邵俊、离子极化导论合肥:安徽教育出版社,1985:54) [2] Thasatti S. Faraday Trans, 1972; 168: 229 [3] Wang G C, Sun Y H, Zhong B. Chem Bull, 1998; 3: 51(王贵昌,孙予罕,钟炳化学通报,19982 3:51) [4] Littel C. Introduction to Solid State Physics. New York:Wileyt 1976: 296 [5] Xu X, Wang N. Zhang Q. Surf Sci, 1992; 274: 378 [6] Swaddle T W. Inorganic Chemistry. New York: AcademicPress, 1997: 89 [7] Yang P, Gao X H. Pmperty-Stoicture-Chemical Bo nding.BeiJing: High Education Press, 1987: 404(杨频,高孝恢性能-结构-化学键北京:高等教育出版社,1987:404) [8] Wuhan University, Jinn University et al. Inorganic Chemistry (I). Beijing: High Education Press, 1986: 117武汉大学,吉林大学等校编无机化学(上册).北京:高等教育出版社出版, 1986: 117) [9] Lide D R. CRC Handbook Of Chemical and Physics. 66th,Florida: CRC Press, 1985-1986: E-86-87 [10] Pauling L ed, Lu J X, Huang Y Z, Zeng G Z, Chen Y Ztrans. The Nature of the Chemical Bond. Shanghai: UnivPress, Ithaca, 1966: 93((美)L鲍林著,卢嘉锡,黄耀曾,曾广植,陈元柱化学键的本质.上海:上海科学技术出版社,1966:93)q |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|