| 原位自反应合成A1N粉体 |
| 金海波 邹宗树 |
| 清华大学新型陶资与精细工艺国家重点实验室; 北京 100084 |
|
引用本文:
金海波; 邹宗树 . 原位自反应合成A1N粉体[J]. 金属学报, 2000, 36(7): 775-779 .
[1] Slack G A, Tranzili R A, Pohl R O, Vandersande J W. JPhys Chem Solids, 1987; 48: 641 [2] Sheppard L M. Am Ceram Soc Bull, 1990; 69: 1801 [3] Lou V L K, Mitchell T E, Hener A H. J Am Ceram Soc,1985; 68: 49 [4] Juneja J M, Iyengar G N K, Abraham K P. J Chem Thermodyn, 1980; 18: 1025 [5] Ding X Y, Wang W Z. Acta Metall Sin, 1994; 30: B444 (丁学勇,王文忠,金属学报,1994;30:B444) [6] Jin H B.Master,Thesis,Northeastern University; Shenyang, 1999 (金海波,东北大学硕士学位论文,沈阳,1999)9 |
|