关于钢铁工业废钢资源的基础研究 |
陆钟武 |
东北大学材料与冶金学院; 沈阳 110006 |
|
引用本文:
陆钟武 . 关于钢铁工业废钢资源的基础研究[J]. 金属学报, 2000, 36(7): 728-734 .
[1] Zhou C D, Tao J. Iron Steel, 1997; 32(Suppl.): 253(周传典.陶晋,钢铁、1997:32增刊〕:253) [2] Lu Z W, Xie A G, Cai J J, Zhai Q G, Meng Q S. IronSteel, 1997; 32(Suppl.): 1(陆钟武,谢安国,蔡九菊,翟庆国,孟庆生钢铁,1997; 32(增刊):1) [3] Steel Statistical Yearbook 1998. International Iron andSteel Institute, Committee on Economics Studies, Brussels, December, 1998: 55 [4] Kavanagh L. Steel Industry Technology Roadmap. American Iron and Steel Institute, 1998: 52 [5] Graedel T E, Allenly B R. Industrial Ecology. PrenticeHall, New Jersey, 1995: 114 [6] Aelion V, Castells F, Veroutis A. Environ Prog, 1995; 14:1930 |
|