H0Cr17Ni6Mn3钢丝电塑性拉拔的研究 |
姚可夫 方威 |
清华大学机械工程系; 北京 100084 |
|
引用本文:
姚可夫; 方威 . H0Cr17Ni6Mn3钢丝电塑性拉拔的研究[J]. 金属学报, 2000, 36(6): 630-633 .
[1] Troitskii O A Lichtman V I Doki Akad Nauk SSSR 1963;148:332 [2] Ohzaki K,Kagawa M,Conrad H.Scr,Metall,1978:121063 [3] Conrad H,Karam N, Mannan S L Scr,Metall,1983;17:411 [4] Troitskii O A Mate, Sci Eng, 1985; 75A 37 [5]Sprecher A F,Mannan S L,Conrad H.Acta Metall,1986;34:1145 [6] Zheng M X,Ta ng G Y,Zhu Y H,Zhang H T J TsinghuaUniversity,1998;38:28(郑明新,唐国翌,朱水华、张华堂清华大学学报。1998;38:28) [7] Yao K F Wang J, Zheng M X、 Yu P, Zhang H, Fang W.UMRS-ICAM’99 Jun,13-18, 1999: 376 [8] Sheng Y F, Guo X N, Zhans K, Li S L, Zhou B L Mater,Sci Eng,1998; 63:4(沈以赴,郭小楠,张坤,李顺林,周本濂材料科学与工程,1998 63:4) [9] Qin R S Zhou B L J Mate, Res; 1997 69: 11(秦荣山,周本濂 材料研究学报,19972 69:11) |
|