| 冶金熔渣热力学性质的SReS模型 |
| 唐恺 蒋国昌 |
| 北京科技大学理化系; 北京 100083 |
|
引用本文:
唐恺; 蒋国昌 . 冶金熔渣热力学性质的SReS模型[J]. 金属学报, 2000, 36(5): 502-506 .
[1] Lumsden J. In: Pierre G R St ed, Physical Chemistry ofProcess Metallurgy, Part I,Interscience, New York, 1961:165 [2] Ban-Ya S. ISIJ Int, 1993; 33: 2 [3] Jahanshahi S, Wright S. In: 4th International Condrenceon Molten Slags and Fluxes, Sendai,Japan,ISIJ,1992:61 [4] Li H, Morrios A, Robertson G. Metall Mater Trans,1998;B29: 1181 [5] Xu K D, Jiang G C, Huang S P, You J L. Set China,1998;E28: 499(徐匡迪,蒋国昌,黄世萍,尤静林.中国科学,1998;E28:499) [6] Zhang X B, Jiang G C, Tang K, Ding W Z, Xu K D.Calphad, 1997; 22: 301 [7] Tang K, Xu J L, Ding W Z, Zhang X B, Jiang G C, Xu KD. In: 8th INFACON, Beijing, China Metal Society, 1998:284 [8] Rein R H, Chipman J. Trans TMS-AIME, 1963; 227:1193 [9] Sharma K P, Richardson F D. J Iron Steel Inst, 1962; 200:1372 [10] Atlas S. Verein Deutscher Eisenhuttenleuten VarlagStahleisen B H, Dusseldofr, 1981 [11] Pelton A D, Blander M. Metall Trans,1986; B17: 805 [12] Rao B K P, Gaskell D R. Metall Trans,1981; B12: 311 [13] Aramaki S, Roy R. J Am Cerma Soc, 1962; 45: 229 [14] Tang K. Post Doctoral Research Report, University of Sci-ence and Technology Beijing, 2000(唐 恺.北京科技大学博士后研究报告,2000) [15] Ragavan S, Iyenger G N K, Abraham K P. Trans IndianInst Met, 1980; 3: 51 [16] Tasi T, Muan A. J Am Cerma Soc, 1993; 76: 1472 [17] Schench H, Forhberg M G, Nunninghoff R N. Arch Eisen-huettenwes, 1964; 35: 269K |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|