| 致密FGH95合金的高温变形特性研究 |
| 张麦仓 罗子健 |
| 西北工业大学材料科学与工程学院;西安 710072 |
|
引用本文:
张麦仓; 罗子健 . 致密FGH95合金的高温变形特性研究[J]. 金属学报, 2000, 36(5): 507-510 .
[1] Wang S H. In: Wang S H, Chen H X, Tang A Qeds, Proceedings of the 4th National Condrence on Iso-static Pressing Technology, Beijing: Metallurgical Indus-try Press,1996:1(王声宏.见:王声宏,陈宏霞,唐安青主编,第四届全国等静压学术会议论文集,北京:冶金工业出版社,1996:1) [2] Pfouts W R, Shamblem C E, Moster J S. NASA-CR-159802, 1979: 3 [3] Morra J M, Biederman R R, Tuler F R. In: RiechmanS ed, Soperalloys 1988, The Metallurgical Society, 1988:505 [4] Cul J. Ph D Dissertation, Beijing Institute of Aeronauti-cal Materials, 1995: 25(崔 健.博士学位论文,北京航空材料研究院,1995:25) [5] Zhou J H, Guan K Z. Resistance to Plastic Deformationof Metals. Beijing: Mechanical Industry Press, 1989: 138o |
|