| 机械活化对Al-Ti-C粉料合成反应激活能的影响 |
| 马乃恒 方小汉 |
| 西安交通大学机械工程学院;西安 710049 |
|
引用本文:
马乃恒; 方小汉 . 机械活化对Al-Ti-C粉料合成反应激活能的影响[J]. 金属学报, 2000, 36(11): 1169-1171 .
[1] Ma H H, Fang X H, Liang G Y, Su J Y. Chin J NonferrousMet, 2000; 10: 900(马乃恒,方小汉,梁工英,苏俊义中国有色金属学报,2000;10:900) [2] Ren R M, Yang Z G, Shaw L L. Scr Mated 1998; 38: 735 [3] Ye L L, Liu Z G, Liu S D, Guan M X, Hu Z Q. J MaterRes, 1997; 12: 616 [4] Wu N Q, Lin S, Wu M, Li Z Z. J Mater Sci Technol, 1998;14: 287 [5] Rigaku Co ed. Testing Center Zhejiang University trans.Handbook oj X-Ray Diffraction. Japan, Rigaku Co Ld,1987: 55(理学电机编浙江大学测试中心译X射线衍射手册日本,理学电机株式会社, 1987: 55) [6] Nukami T, Flemings M C. Metall Mater Trans, 1995; A26:1877 [7] Chen J H, Li C R. Thermal Analysis and Its Applications.Beijing: Science Press, 1985: 112(陈镜泓,李传儒.热分析及其应用、北京:科学出版社,1985:112) [8] Forrester J S, Schaffer G B. Metall Mater Trans, 1995;A26: 725U |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|