| CaO-SiO2-TiO2-Al2O3-MgO炉渣中三价和四价Ti氧化物的氧化还原平衡 |
| 薛向欣 段培宁 |
| 东北大学材料与冶金学院;沈阳 110006 |
|
引用本文:
薛向欣; 段培宁 . CaO-SiO2-TiO2-Al2O3-MgO炉渣中三价和四价Ti氧化物的氧化还原平衡[J]. 金属学报, 2000, 36(11): 1172-1174 .
[1] Ma J Y, Sun X W, Diao R S. Theory and Practice forSmelting Process by Means of Blast Furnace with Vanadiferous Titanomagnetite Ore as Raw Materials. Beijing:Metallurgical Industry Press, 2000: 1(马家源,孙希文,刁日升.高炉冶炼钒钛磁铁矿的理论与实践,北京;冶金工业出版社,2000:1) [2] Saito K, Sano N, Matsushita Y. J Iron Steel Inst Jpn,1975: 61: 391s(斋藤健志,佐野信雄,松下幸雄. 铁 钢, 1975; 61: 391s) [3] Ito K, Sano N. J Iron Steel Inst Jpn, 1981; 67: 59(伊藤公久,佐野信雄.铁 钢,1981;67:59) [4] Baxter G P, Lansing J E. J Am Chem Soc, 1920; 42: 419 [5] Xue X X, Che Y C. Z Metallkd, 1994; 6: 391 [6] Miao Z J, Feng M H. Anal Lab, 1983; (4): 33(缪兆佳,冯明华.分析实验室,1983;(4):33) [7] Mori K. Trans Iron Steel Inst, 1969; 4: 409 [8] Xue X X, Li Y, Duan P N. Chin J Nonferrous Met, 1997;5(Suppl.): 32(薛向欣,厉英,段培宁中国有色金属学报,1997;5增刊):32)4 |
|