| Ni-Cr-Al-Y涂层真空热处理过程中元素的行为 |
| 王冰 韩雅芳 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
王冰; 韩雅芳 . Ni-Cr-Al-Y涂层真空热处理过程中元素的行为[J]. 金属学报, 2000, 36(10): 1094-1098 .
[1] Czech N, Juez-Lorenzo M, Kolarik V, Stamm W. SurfCoat Technol, 1998; 108/109: 36 [2] Lih W, Chang E, Wu B C, Chao C H. StEr f Coat Technol,1992; 50: 277 [3] Iwamoto H, Sumikawa T, Nishida K, Asano T, Nishida' M, Araki T. Mater Sci Eng, 1998; A241: 251 [4] Brandl W, Toma D, Grabke H J. Surf Coat Technol, 1998;108/109: 10 [5] Han Y F, Xing Z P, Chaturvedi M C, Xu Q. Mater SciEng, 1997; A239: 871 [6] Brandl W, Grabke H J, Toma D, Kruger J. Surf CoatTechnol, 1996; 86/87: 41 [7] Czech N, Schmitz F, Stamm W. Surf Coat Technol, 1994;68/69: 17 [8] Kolomatsev P T, translated by Ma Z C. Hot-ResistantDiffesion Coatings. Beijing: National Defence industryPress. 1988: 182 著,马志春译.耐热扩散涂层.北 京:国防工业出版社, 1988: 182) [9] Cai Y L,Zheng Y R.Metallographical Study of Super,Al loys.Beijing:National Defence Industry Press,1986:38(蔡玉林,郑运荣.高温合金的金相研究北京:国防工业出版社1986:38) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|