| 亚微米铜循环形变特征研究 |
| 吴世丁 王中光 李广义 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室; 沈阳 110015 |
|
引用本文:
吴世丁; 王中光; 李广义 . 亚微米铜循环形变特征研究[J]. 金属学报, 1999, 35(9): 960-963 .
[1] Suresh S. Fatigue of Materials London:Cambridge Univer-sity Press;1991 [2] Segal V M.Mater Sci Eng.1995;A197:157 [3] Vinogradov A,Kaneko Y,Kitagawa K,Hashimoto S、Stol-yarov V, Valiev R Z Scr Mater.1997;36:1345 [4] Agnew S R Weertman J R. Mater Sci Eng,1998;A244:145 [5] Hahn H,Mondal P.Padmanabhan K A. Nano Struct Mater1997;9:603 [6] Horita Z, Smith D J, Nemoto M,Valiev R Z,Langdon T GJ Mater Res,1998;13:446 [7] Valiev R Z, Kozlov E V.Ivanov Yu F. Lian J Nazarov A A,Baudelet B.Acta Metall Mater.1994;42:2467 [8] Feltner C E. Laird C. Acta Metall,1967;15:1621 [9] Feltner C E,Laird C. Acta Metall,1967;15:1633 |
|