| Cu在Pt(111)面上电结晶的成膜过程研究 |
| 印仁和;曹为民;施文广;孙洁林;毛秉伟;孙世刚 |
| 上海大学化学系;上海嘉定;201800;上海大学化学系;上海嘉定;201800;上海大学化学系;上海嘉定;201800;中国科学院原子核研究所;上海嘉定;201800;厦门大学固体表面物理化学国家重点实验室;厦门;361005;厦门大学固体表面物理化学国家重点实验室;厦门;361005 |
|
| STUDY ON THE PROCESS OF COPPER ELECTRODEPOSITION ON PLATINUM (111) |
| YIN Renhe; CAO Weimin; SHI Wenguang(Department of Chemistry; Shanghai University; Shanghai 201800)SUN Jielin(Institute of Nuclear Research; The Chinese Academy of Sciences; Shanghai 201800)MAO Bingwei; SUN Shigang(State Key Laboratory for Physics Chemistry of the Solid Surface; Xiamen University; Xiamen 361005)Correspondent: YIN Renhe; associate profsson Tel: (021)59532932-272; Fax: (021)59529932;E-mail: papayaly online. sh. ch |
引用本文:
印仁和;曹为民;施文广;孙洁林;毛秉伟;孙世刚. Cu在Pt(111)面上电结晶的成膜过程研究[J]. 金属学报, 1998, 34(8): 892-896.
,
,
,
,
,
.
STUDY ON THE PROCESS OF COPPER ELECTRODEPOSITION ON PLATINUM (111)[J]. Acta Metall Sin, 1998, 34(8): 892-896.
1印仁和,曹为民,郭也平,计慧芬,周天健,秦勇,王葛亚.电化学,1997;3:252 (Yin R H, Cao W M, Guo Y P, Ji H F, Zhou T J, Qin Y, Wang G Y. Electrochemistry; 1997; 3: 252) 2Batina N, will T, Kolb D M. Faraday Discuss Chem Soc, 1992; 94: 93 3谢兆雄,毛秉伟,卓向东,穆纪千,田昭武.电化学,1996; 2:164 (Xi Z X, Mao B W, Zhuo X D, Mu J Q, Tian Z W. Electrochemistry 1996; 2: 164) 4常光幸矣,林安德.日本金属学会会报,1992;31:849 (Jyoko Y,hayashi Y.Bull Jpn Inst Met,1992; 31:849 5 Azgile C,Rhead G E.Surf Sci Rep,1989;10:277 6李宗全.物理,1989;18:715(Li Z Q. Physics, 1989; 18: 715) |
|