| 仿晶型铁素体表面浮凸的扫描隧道显微镜研究 |
| 薄祥正;方鸿生 |
| 清华大学材料科学与工程系;北京;100084;清华大学材料科学与工程系;北京;100084 |
|
| STUDY OF THE SURFACE RELIEF EFFECTS ASSOCIATED WITH GRAIN BOUNDARY ALLOTRIOMORPHS BY SCANNING TUNNELING MICROSCOPY |
| BO Xiangzheng; FANG Hongsheng( Departmetn of Materials Science and Engineering; Tsinghua University; Beijing; 100084)Correspondent: BO Xiangzheng; Tel: (010)62782361; E-mail: fhs - dms tsinghua. edu. cn. |
引用本文:
薄祥正;方鸿生. 仿晶型铁素体表面浮凸的扫描隧道显微镜研究[J]. 金属学报, 1998, 34(8): 807-812.
,
.
STUDY OF THE SURFACE RELIEF EFFECTS ASSOCIATED WITH GRAIN BOUNDARY ALLOTRIOMORPHS BY SCANNING TUNNELING MICROSCOPY[J]. Acta Metall Sin, 1998, 34(8): 807-812.
1 Dube C A, Aaronson H I, Mehl R F. Rev Met, 1958; 55: 201 2 Aaronson H I. In: Zackey V F, Aaronson H I eds., Decomposition of Anstenite by Diffusional Processes.New York: Interscience Publishers, 1962: 387 3 Aaronson H I, Laird C, Kinsman K R. Phaae Transformations, Metals Park, Ohio: ASM, 1970: 313 4 Watson J D, McDougall P G. Acta MetaIl, 1973; 21: 961 5 Kinsman K R, Eichen E, Aaronson H I. Metall Trans, 1975; 6A: 303 6 Hall M G, Aaronson H I. Metall Moter Trans, 1994; 25A: 1923 7 薄祥正,方鸿生,王家军,王峥华金属学报, 1998; 34: 345(Bo X Z, Fang H S, Wang J J, Wang Z H. Acta Metall Sin, 1998; 34: 345) 8 Christian J W. In: Zackey V F and Aaronson H I eds., Decomposition of Austenite by Diffusional Proscesses.New York: Interscience, 1962: 371 9 Christian J W. Metall Mater Trans, 1994; 25A: 1821 10 Kurdjumow G V, Sachs G. Z Phys, 1939; 64:325 11 Aaronson H I, Furuhara T, Rigsbee J M, Reynolds W T Jr, Howe J M. Metall Trans, 1990; 21A: 2369 12 Furuhara T, Maki T. Metall Trans, 1992; 33: 734 13 Aaronson H I, Russell K C. In: Aaronson H I, Laughlin D E, Sekerka R F, Wayman C M eds., Proc Int Confon Solid-to-Solid Phase fTransformations. Warrendale, PA: TMS-AIME, 1994: 371 14 Binnig G, Rohrer H, Gerber Ch, Weibel E. Phys Rev Lett, 1982; 49: 57 15 Binnig G, Rohrer H. Surf Sci, 1983; 126: 236 16 Yamamoto M, Fuisawa T, Saburi T, Kurumizawa T, Kusao K. Surf Sci, 1992; 266: 289 17 Fang H S, Wang J J, Yang Z G, Li C M, Zheng Y K, Li C X. Metall Mater Trans, 1996; 27A: 1535 18 Wang J J, Fang H S, Zheng Y K, Yang Z G. ISIJ Int, 1995; 35: 992 19 Yang Z G, Fang H S, Wang J J, Li C M, Zheng Y K. Phys Rev, 1995; B52: 7879 20 Swallow E, Bhadeshia H K D H. Mater Sci Technol, 1996; 12: 121 21 Bo X Z, Fang H S, Wang J J. Scri Mater 1997; 37: 555 22 Bradley J R, Rigsbee J M, Aaronson H I. Metall Trans, 1977; 8A: 323 23 Clark H M, Waymun C M. Metall Trans, 1977; 8A: 206 24 Furuhara T, Aaronson H I. Acta Metall Mater, 1991; 39: 2887 25 Furuhara T, Ogawa T, Maki T. Scri Mater 1996; 34: 381 26 Hall M G, Aaronson H I, Kinsman K R. Surf Sci, 1972; 31: 257 27 Russell K C, Hall M G, Kinsman K R, Aaronson H I. Metall Trans, 1974; 5: 1503 28 Howe J M. Metall Mater Trans, 1994; 25A: 1917 29 Aaronson H I, Wells C. Trans AIME 1956; 206: 1216 30 Aaronson H I, Spanos G, Masamura R A, Vardiman T G, Moon D W, Menon E S K, Hall M G. Mater Sci Eng, 1995; B32: 107 |
|