Please wait a minute...
金属学报  1998, Vol. 34 Issue (4): 412-415    
  论文 本期目录 | 过刊浏览 |
Co-Nb/Cr磁性多层膜的振荡耦合
娄坚鑫;颜世申;刘宜华
山东大学物理系;济南;250100;山东大学物理系;济南;250100;山东大学物理系;济南;250100
OSCILLATORY COUPLING OF THE Co-Nb/Cr MULTILAYERED FILMS
LOU Jianxin; YAN Shishen; LIU Yihua (Department of physics; Shandong University; Jinan 250100)
引用本文:

娄坚鑫;颜世申;刘宜华. Co-Nb/Cr磁性多层膜的振荡耦合[J]. 金属学报, 1998, 34(4): 412-415.
, , . OSCILLATORY COUPLING OF THE Co-Nb/Cr MULTILAYERED FILMS[J]. Acta Metall Sin, 1998, 34(4): 412-415.

全文: PDF(394 KB)  
摘要: Co—Nb/Cr磁性多层膜由高频溅射方法制得由振动样品磁强计测量作品的磁性能在2.67Pa溅射氩气压下,发现样品随Cr层厚度增加,铁磁层间出现铁磁性和反铁磁性的耦合振荡,饱和磁化强度Ms基本保持不变,而在0.67Pa溅射氩气压下,样品的饱和磁化强度Ms发生了振荡,这可能与其铁磁层中顺磁分量振荡变化有关.
关键词 磁性多层膜铁磁耦合反铁磁耦合    
Abstract:Co-Nb/Cr multilayered films were prepared with the rf-sputtering method. The magnetic properties of the samples were studied by a micropro cessor-controlled vibrating-sample magnetometer. When the charging Ar pressure PAr=2.67 Pa, an oscillation between ferromagnetic and antiferromagnetic coupling with the thickness of Cr layers was found, and the spontaneous magnetization Ms remains constant basically. When PAr=0.67 Pa, the value of Ms shows an oscillatory behaviour, which may be related to the oscillatory variation of the paramagnetic component in the ferromagnetic layers.
Key wordsmuiltilayered film    ferromagnetic coupling    antiferromagnetic coupling
收稿日期: 1998-04-18     
基金资助:国家自然科学基金!59392800
1 Grunberg P, Schreiber R, Pang Y, Brodsky M B, Sowers H. Phys Rev Lett, 1986; 57: 2442
2 Barthlmy A, Fert A, Baibich M N, Hadjoudj S, Petroff F, Etienne P, Cabanel R, Lequien S, Nguyen Van Dan F, Creuzet G. J Appl Phys, 1990; 67: 5908
3 Parkin S S P, Bhadra R, Roche K P. Phys Rev Lett, 1991; 66: 2152
4 Celinski Z, Heinrich B. J Magn Magn Maten 1991; 99: L25
5 Parkin S S P, More N, Roche K P. Phys Rev Lett, 1990; 64: 2304
6 Qiu Z Q. Pearson J, Berger A, Bader S D. Phys Rev Lett, 1992; 68: 1398
7 FuB A, Demokritov S, Grunberg P, Zinn W. J Magn Magn Maten 1992; 103: L221
8 Levy M, Ounadjela K, Zhang S, Wang Y, Sommers C B, Fert A. J Appl Phys, 1990; 67: 5914
9 Bruno P, Chappert C. Phys Rev Lett, 1991; 12: 1602
10 Toscano S, Briner B, Hopster H, Landolt M. J Magn Magn Mater, 1992; 114: L6
11 Liu Y H, Zhang Y M, Yan S S, Ma X D. Phys Rev, 1993; B8: 10266
12 谭春雨, 夏日源, 张汝贞, 刘吉田, 刘向东, 许炳章, 李淑英, 陈友鹏, 绑淑芝. 山东大学学报, 1993; 28: 189(Tan C Y, Xia Y Y, Zhang R Z, Liu J T, Liu X D, Xu B Z, Li S Y, Chen Y P, Zhang S Z. i Shandong Uni,1993; 28: 189)
13 Baibich M N, Broto J M, Fert A, Nguyen Van Dan F, Petroff F, Etienne P, Creuzet G, niederich A, ChazelasJ. Phys Rev Lett, 1988; 61: 2472
No related articles found!