| 剪切速率增稠半固态合金浆料的流变力学模型 |
| 陈晓阳;毛卫民;钟雪友 |
| 北京科技大学铸造研究所;北京;100083;北京科技大学铸造研究所;北京;100083;北京科技大学铸造研究所;北京;100083 |
|
| RHEOLOGICAL MECHANICS MODEL OF SHEAR RATE THICKENING THE BEHMIOR OF SEMISOLID SLURRISS |
| CHEN Xiaoyang;MAO Weimin;ZHONG Xuegou (Institute of Casting; University of Science and Technology Beliing; Beijing 100083) |
引用本文:
陈晓阳;毛卫民;钟雪友. 剪切速率增稠半固态合金浆料的流变力学模型[J]. 金属学报, 1998, 34(2): 179-183.
,
,
.
RHEOLOGICAL MECHANICS MODEL OF SHEAR RATE THICKENING THE BEHMIOR OF SEMISOLID SLURRISS[J]. Acta Metall Sin, 1998, 34(2): 179-183.
1Joly P A, Merhraian R.J Mate, Sci 1976; 11: 1393 2Flemings M C.Metall Trans A,1991;22A:957 3Ito Y,Flemings M C,Cornie J A.Nature and Properties of Semi-Solid Materials, Warrendade,PA:TEM, 1992; 3 4Rice J R,J Appl Mech,1970;9:728 5 Alers W, Overbeek J T G.J Col Sci, 1960; 15: 489 6Kumar P,Martin C L;Brown S B.Acta Metall,1994;4:3595 7Frankel N A, Acrivos A. Chem Eng Sci 1967; 22: 847 8Martin C L, Kumar P, Brown S B. Acta Metall, 1994; 42: 3603 9Nguyen T G, Favier D, Suery M. Int J Plast, 1994; 10: 693- |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|