| 关于X射线衍射法测定微观应力的表征值的讨论 |
| 张定铨;何家文 |
| 绍兴文理学院;绍兴;312000;西安交通大学金属材料强度国家重点实验室;西安;710049 |
|
| ON CHARACTERIZATION OF MICROSTRESS MEASURED BY X-RM DIFFRACTION |
| ZHANG Dingquan(Shaoxing College of Arts and Sciences; Shaoxing 312000)HE Jiawen(State Key Laboratory for Mechanical Behavior of Materials; Xi'an Jiaotong University; Xi'an 710049)Correspondent:ZHANG Dingquan; associate professor;Tel: (O575)8067050-2812; Fax. (0575)8067917;E-mail: ZX9915@163.NetManuscript received 1998-02-09; in revised form 1998-07-10 |
引用本文:
张定铨;何家文. 关于X射线衍射法测定微观应力的表征值的讨论[J]. 金属学报, 1998, 34(12): 1273-1278.
,
.
ON CHARACTERIZATION OF MICROSTRESS MEASURED BY X-RM DIFFRACTION[J]. Acta Metall Sin, 1998, 34(12): 1273-1278.
1 1935;4(6):688(Daviginkof N N Industrial Laboratory, 1935i 4(6): 688) 2 Greenough G B.J Iron Steel Iust, 1951; 169: 235 3辛岛诚一,岛谷幸治,一柳肇材料,1963;12:848(Karashim S, Shimatani K, Hitotssuyanagi H. Material, 1963; 12: 848 4 Bollenrath P, Hank V, Ohly W. Areh Eisewhuettenwes, 1970; 41: 445 5 Garrod RI, Hawkes G A. Br J Appl Phys, 1963; 14: 422 6Macherauch E,Wohlfahrt H.Wolfstieg V.Haerterei-Tech Mitt,1973;28:201(Macherauch E, WOhlfahrt H, Wolfstieg V. Trans Hardening Technol,1973; 28: 201) 7Eigenmann B,Macherauch E,Mat-wiss werkstofftech,1995;26:148(Eigenmann B,Macherauch E.Mater Sci Technol,19952 26:148) 8Cullity B D. Ady X-Ray Anal, 1976; 20: 259 9康飞宇,唐遒泳,刘秀瀛.机械强度,19912 13(1:22(Kang F Y, Tang N Y, Liu X Y.J Mech Strength ,1991; 13(1): 22) 10Scholtes B.Eigenspannungen in Mechanisch Randschichtverformten Werkstoffzustaenden,Oberurel:DGMInformationsg6sellschaft Verlag, 1991: 120(Scholtes B,Residual Stresser in Mehanic surface-deformed Materials.Oberursel:GSM Information Society Press, 1991: 120) 11张建中,冯忠信,张定铨,胡志忠,陈新增,胡奈赛西安交通大学学报,1982;16(1):23(zhang J z,Feng z x,zhang D Q,Hu z z,chen x z,Hu N s.J xi’an Jiaotong Univ 1982; 16(1):23)3 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|