Al-0.53Zn合金近快速定向凝固条件下的胞晶间距选择 |
冯坚;黄卫东;林鑫;李涛;薛玉芳;周尧和 |
西北工业大学凝固技术国家重点实验室;西安;710072;西北工业大学凝固技术国家重点实验室;西安;710072;西北工业大学凝固技术国家重点实验室;西安;710072;西北工业大学凝固技术国家重点实验室;西安;710072;西北工业大学凝固技术国家重点实验室;西安;710072;西北工业大学凝固技术国家重点实验室;西安;710072 |
|
CELLULAR SPACING SELECTION OF Al-0.53Zn ALLOY UNDER NEAR-RAPID DIRECTIONAL SOLIDIFICATION CONDITION |
FENG Jian; HUANG Weidong; LIN Xin; LI Tao; XUE Yeing; ZHOU Yaohe(State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072)Correspondent:FENG Jian; Tel: (O29)-8494001; Fax: (0E9)-8491544;E-mail. Huang@nwpu.edu.cn Manuscript received 1998-03-10; in revised form 1998-06-01 |
引用本文:
冯坚;黄卫东;林鑫;李涛;薛玉芳;周尧和. Al-0.53Zn合金近快速定向凝固条件下的胞晶间距选择[J]. 金属学报, 1998, 34(12): 1267-1272.
,
,
,
,
,
.
CELLULAR SPACING SELECTION OF Al-0.53Zn ALLOY UNDER NEAR-RAPID DIRECTIONAL SOLIDIFICATION CONDITION[J]. Acta Metall Sin, 1998, 34(12): 1267-1272.
1Warren J A, Langer J S. Phys Rev, 199O; A42: 3518 2 Warren J A, Langer J S. Phys Rev 1993; E47: 2702 3Lu shuzu,Hunt J D.J Cryst Growth,1992;123:17 4 Hunt J D, Lu Shuzu. Metall Mater Trans, 1996; A27: 611 5 Han S H,Trivedi R.Acta Metall Mater,1994242:25 6 Quested P N,McLean M.Mater,Sci Eng,1984;65:171 7 Chopra M A, Tewari S N. Metall Trans,1991; A22: 2467 8 Huang Weidong,Geng Xingguo,ZHou Yaohe,J Cryst Growth,1993;134:105 9 Ding G L, Huang W D, Huang X, Lin X, Zhou Y H. Acta Mater 1996; 44: 3705 10林鑫,黄卫东,潘清跃,丁国陆,薛玉芳,周尧和.金属学报,1997; 33: 1140 (Lin X, Huang W D, Pan Q Y, Ding G L, Xue Y F, Zhou Y H. Acta Metall Sin, 1997; 33: 1140) 11 Kurzw,Gioranola B,Trivedi R,Acta Metall,1986;34:823 12 Boettinger W J,Bendersky L A,Coriell R J.Schaefer R J.Biancaniello F S.J Cryst Growth,1987;80:17 13 Juarez-Islas J A,Jones H ,Kurz W .Mater Sci Eng ,1988;98:201 14 Juarez-Islas J A,Joues H.Acta Metall , 1987; 35:499 15 Gremaud M,Carrard M,Kurz w.Acta Metall Mater,1990;38:2587 16 Kurz W, Fisher D J Acta Metall, 1981; 29: 11 17 Trivedi R.Kurz W.Int Mater Rev,19942 3g:49 18 Hunt J D,Solidification and Casting of Metals London:The Metals Society ,1979:3 19 Sato T, Ito K, Ohira G Trans Jpn Inat Met, 1980; 21: 441 20 Lu S Z, Hunt J D, Gilgien P, Kurz W. Acta Metall Matet 1994; 42: 1653 |
|