| 液态反应法制备TiC_p增强铸造Fe-Cr-Ni基复合材料 |
| 惠希东;王执福;杨院生;吴欣强;陈熙琛 |
| 中国科学院金属研究所;沈阳;110015;山东工业大学济南;250061;山东工业大学;济南;250061;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院物理研究所;北京;100080 |
|
| CAST Fe-Cr-Ni MATRIX COMPOSITE REINFORCED BY TiC_p SYNTHESIZED WITH LIQUID STATE IN SITU PROCESS |
| HUI Xidong; WANG Zhifu; YANG Yuansheng; WU Xinqiang; CHEN Xichen (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Shandong University of Technology; Jinan 250061)(Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)Correspondent: HUI Xidong; Tel: (024)23843531-55963; Fax: (024)23891320 |
引用本文:
惠希东;王执福;杨院生;吴欣强;陈熙琛. 液态反应法制备TiC_p增强铸造Fe-Cr-Ni基复合材料[J]. 金属学报, 1998, 34(10): 1115-1120.
,
,
,
,
.
CAST Fe-Cr-Ni MATRIX COMPOSITE REINFORCED BY TiC_p SYNTHESIZED WITH LIQUID STATE IN SITU PROCESS[J]. Acta Metall Sin, 1998, 34(10): 1115-1120.
1 Kaufman M. In: Gell M ed., Proc 5th Int Symp On Smpnalloys, Warrendale, PA: TMS-AIME 1984: 43 2 Kattamis T Z, Suganuma T. Mdter Sci Eng, 1990; A128: 241 3 Skolianos S, Kattamis T Z, Chen M. Mater Sci Eng, 1994; A183: 195 4 Pyzalla A, Genzel C, Reimers W. Mater Sci Eng, 1996; A212: 130 5 Hui X D, Wang Z F, Chen X C. Met Phys Adv Technol, 1996; 18(9): 58 6 惠希东.山东工业大学博士学位论文,1997(Hui X D. PhD Thesis, Shandong University of Technology 1997) 7 Williams W S, Schaal E E. J APPl Phys, 1962; 33: 955 8 Hollex G E. Mater Sci Eng, 1969; 3: 121 |
|