| 熔滴冲击力对MIG焊接熔池表面形状的影响 |
| 武传松;L.Dorn |
| 山东工业大学;济南;250061;柏林工业大学;德国 |
|
| THE INFLUENCE OF DROPLET IMPACT ON METAL INERT GAS WELD POOL GEOMETRY |
| WU Chuansong (Shandong University of Technology; Jinan 250061); L. DORN (Berlin Technical University; Germany) |
引用本文:
武传松;L.Dorn. 熔滴冲击力对MIG焊接熔池表面形状的影响[J]. 金属学报, 1997, 33(7): 774-780.
,
.
THE INFLUENCE OF DROPLET IMPACT ON METAL INERT GAS WELD POOL GEOMETRY[J]. Acta Metall Sin, 1997, 33(7): 774-780.
1TsaoKC,WuCS.WeldJgl988;67:70—s 2 Wu C S.Eng Comput,1992;9:529 3Pardo E, Weckamn D C. Metall Trans, 1989; 20B: 937 4 TekriwalP,MazumderJ.Weld J,1988;67:150—s 5曹振宁,武传松,吴林.金属学报,1994;30:B537 6 Kim J-W,Na S-J.Trans ASME:JEnglnd,1994;116:78 7KetterRL,Prawel S R.Mode。Methods of Engineering Computation New York:McGraw—Hill,1969:38 8 Waszink J H,van den Heuvel G J P M.Weld J,1982;61:269—s 9 Essers W G,Walter R.Weld J,1981;60:37—s 10Liguo E, Wu L, Zhang J. Chin Weldg 1993; 2: 55 11 LinML,EagerTW.MetallTrans,1986;17B:601 12Smart H B. ASM Handbook. Vol.6, Metals Park, Ohio: ASM International, 1993: 25l |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|