| Vogel—Fulcher定律与玻璃转变温度的关系 |
| 蒋青;徐晓亚;赵明 |
| 吉林工业大学;长春;130025;吉林工业大学;长春;130025;吉林工业大学;长春;130025 |
|
| RELATIONSHIP BETWEEN VOGELFULCHER LAW AND GLASS TRANSITION TEMPERATURE |
| JIANG Qing;XU Xiaoya;ZHAO Ming (Jilin University of Technoloasl; Changchun 130025) |
引用本文:
蒋青;徐晓亚;赵明. Vogel—Fulcher定律与玻璃转变温度的关系[J]. 金属学报, 1997, 33(7): 763-768.
,
,
.
RELATIONSHIP BETWEEN VOGELFULCHER LAW AND GLASS TRANSITION TEMPERATURE[J]. Acta Metall Sin, 1997, 33(7): 763-768.
1Zallen R. The Phyjlcs ofAmorrkous Solids. New York: A Whey—Interscience Publication, 1983: 3 2Johnson W L.Prog Mater Sci,1986;30:81 3Saslow W S.Phys Rev,1988;37B:676 4 BruningR,Samwer J H.Phys Rev,1992;46B:318 5 KloseG,FechtJH.Mater Sci Eng,1994;A179/180:77 6蒋青,赵明,吕晓霞.材料研究学报, 1997; 11: 187 7 LuckR,JiangQ,Predel B R.J Non-Cryst Solids,1990;117-118:911 8Shi F G.J Mater Res, 1994;9: 1908 9Kauzmann W. Chem Rev, 1948; 43: 21 |
|