| 亚快速凝固中枝晶→细胞晶转变的理论研究 |
| 耿兴国;傅恒志 |
| 西北工业大学;西安;710072;中国科学院国际材料物理中心;沈阳;110015;中国科学院国际材料物理中心;沈阳;110015 |
|
| THEORETICAL RESEARCH OF TRANSITION FROM DENDRITE TO FINE CELL IN SUB-RAPID SOLIDIFICATION |
| GENG Xingguo; FU Hengzhi(Northwestern Polytechnical University; Xi'an 710072) (International Centre .for Materials Physics; Chinese Academy of Sciences;Shenyang 110015) |
引用本文:
耿兴国;傅恒志. 亚快速凝固中枝晶→细胞晶转变的理论研究[J]. 金属学报, 1997, 33(7): 673-676.
,
.
THEORETICAL RESEARCH OF TRANSITION FROM DENDRITE TO FINE CELL IN SUB-RAPID SOLIDIFICATION[J]. Acta Metall Sin, 1997, 33(7): 673-676.
1 Mullins W W,Sekerka R F.J Appl Phys,1964;35:444 2 Boettinger W J, Shechtman D,Schaefer R J,Biancaniello F S.Metall Trans,1984;15A:553 Trivedi R,Kurz W. Acta Metall Mater,1994;42:15 4 Trivedi R, Sekhar J A, Seetharaman V. Metall Trans, 1989; 20A: 769 5 Kotler G R, Tiller W A. ln: Peiser H S ed, Crystal Growth, Oxford: Pergamon, 1967: 721 6 Trivedi R.J Crust Growth, 1980; 48: 93 7 Ivantsov G P.Dokl Akad Nauk SSSR,1947;58:567 8 Trivedi R, Somboonsuk K. Acta Metall, 1985; 33:1061 9 Kattamis T Z, Flemings M C. TMS AIME, 1965; 233: 992 10 Langcr J S,Miller-Krumbhaar H.Acta Metall,1978;26:1681,1689,1697 11 Juarez—Islas J A,Jones H,Kurz W Mater Sci Eng,1988;98:201 12俞露.西北工业大学硕士学位论文,1996 13 Kurz W,Fisher D J.Acta Metall,1981;29:11 |
|