| CVD法合成SiC晶须的实验研究 |
| 陈卫武;邹宗树;王天明 |
| 东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006 |
|
| NEW PROCESS FOR SYNTHETIC SiC WHISKERS BY CVD |
| CHEN Weiwu;ZOU Zongshu; WANG Tianming(Northeastern University; Shenyang110006) |
引用本文:
陈卫武;邹宗树;王天明. CVD法合成SiC晶须的实验研究[J]. 金属学报, 1997, 33(6): 643-649.
,
,
.
NEW PROCESS FOR SYNTHETIC SiC WHISKERS BY CVD[J]. Acta Metall Sin, 1997, 33(6): 643-649.
1Nair S V, Tien J K, Bates R C. Int Met Rev, 1985: 30: 275 2Wei George C,Becher Paul F.Am Ceram Soc Bull,1985:64:298 3韩敏芳,李伯涛,郭梦熊.材料工程,1995;(9): 3 4 Pickard S M,Derby B,Feest E A.J Mater Sci,1991;26:6207 5 Wada H,Wang M J,Tien T Y.J Amer Ceram Soc、1988;71:837 6Klinger K,Straus E L,Lomarek K L.J Amer Ceram Soc、1966;7:49 7 Chrysanthou A,Grieveson P,Jha A.J Mater Sci,1991:26:3463 8徐永东,张立同,张湛.复合材料学报,1995;21:12 9陈康华,肖泽强.硅酸盐学报,1995;5:23 10 Saito M,Nagashima S,Kato A.J Mater Sci Lett.1992;11:373 |
|