|
|
|
| [Co/Ti],[Co/Cu(Ni)]多层膜的结构与磁性 |
| 吴萍;姜恩永;王存达;白海力;刘裕光;王合英 |
| 天津大学;天津;300072;天津大学;天津;300072;天津大学;天津;300072;天津大学;天津;300072;天津大学;天津;300072;天津大学;天津;300072 |
|
| MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS |
| WU Ping;JIANG Enyong; WANG Cunda; BAI Haili; LIU Yuguang; WANG Heying(Tian jin University; Tianjin; 300072) |
引用本文:
吴萍;姜恩永;王存达;白海力;刘裕光;王合英. [Co/Ti],[Co/Cu(Ni)]多层膜的结构与磁性[J]. 金属学报, 1997, 33(6): 625-630.
,
,
,
,
,
.
MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS[J]. Acta Metall Sin, 1997, 33(6): 625-630.
1 Parkin S S P,More N,Roche K P.Phys Rev Lett,1990;64:2304 2Barthelemy A,Fert A,Baibich M N,HadjoudjS,Petroff F.J Appl Phys,1990;67:5908 3 Parkin S S P,Bhadra R,Roche K P.Phys Rev Lett,1991;66:2152 4 Inomata K,Yusu K,Saito Y.Mater Sci Eng,1995;B31:41 5Qiu Z Q,Pearson J,Berger A,Bader S D.Phys Rev Lett,1992;68:1398 6 Fub A,Demokritov S,Grunberg P.J Magn Magn Mater,1992:103:L221 7Liu Y H, Zhang Y M,Yan S S, Ma X D. Phys Rev, 1993; B48: 10266 8 Shi Z P and Klein B M.Phys Rev,1995;B52:12516 9Bobo J F,Hennet b,Piecuch M.J Magn Magn Mater,1995;140-144:587 10 Bruno P,Chappert C.Phys Rev Lett.1991;67:1602 11 XU Y B, Lu M, Bie Q S, Zhai Y, Jin Q Y, Zhu X B, Zhai H R. J Magn Magn Mater, 1995;140—144: 581 12 Fabian D T. Band structure spectroscopy ofmetals and alloys.London: Academic Press, 1973: 63,679 13 Leevwen R V,England C D,Dutcher J R,Falco C M.J Appp Phys,1990;67:4910F |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|