    					| 环境保护对炼铁技术发展的影响(英文) | 
  					 
  					  										
						| 卢维高 | 
					 
															
					| McMasterUniversity;Hamilton;Ontario;Canada | 
					 
										
						 | 
					 
   										
    					| THE IMPACT OF THE ENVIRONMENTAL CONCERNS ON THE DEVELOPMENT OF IRONMAKING TECHNOLOGY | 
  					 
  					  					  					
						| W-K.LU (McMaster University; Hamilton; Ontario; Canada) | 
					 
														 
				
				引用本文: 
				
								卢维高. 环境保护对炼铁技术发展的影响(英文)[J]. 金属学报, 1997, 33(2): 207-212.	
																												 																								 . 
				THE IMPACT OF THE ENVIRONMENTAL CONCERNS ON THE DEVELOPMENT OF IRONMAKING TECHNOLOGY[J]. Acta Metall Sin, 1997, 33(2): 207-212.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																  1 Proccedings of 3rd International Ironmaking Congress, Sept. 16- 18, 1996, Gent, Belgium. Five papers inSession 6: Sinter Plant environmental Control pp. 151 - 183. 2 Proceedings of 3rd International Cokemaking Congress, Sept. 16- 18, 1996. Gent, Belgium. Four papersin Session 7. Environmental Control in Coking Plants: water Six papers in Session 9: EnvironmentalControl in Coking Plants: Air and By-Products pp. 130- 190. 3 W-K.Lu and M.G.Ranade, ISIJ Int 3 (1991) pp.395-405. 4 Alternative Irons Defined and Explained, New Steel Magazine, October, (1996) 68-72. A Chilton publi-cation.x | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |