现代织构分析的进展
梁志德
东北大学;沈阳;110006
PROGRESS IN MODERN TEXTURE ANALYSIS
LIANG Zhide (Northeastern University; Shenyang 110006)
引用本文:

梁志德. 现代织构分析的进展[J]. 金属学报, 1997, 33(2): 133-142.
. PROGRESS IN MODERN TEXTURE ANALYSIS[J]. Acta Metall Sin, 1997, 33(2): 133-142.

全文: PDF(819 KB)  
摘要: 本文系统阐述了材料现代织构分析的进展。
关键词 : 织构分析,  简ODF,  真ODF,  织构矢量    
Abstract:The progress in modern texture analysis was systematically elucidated in this paper.
Key words: texture analysis    reduce ODF    true ODF    texture vector
收稿日期: 1997-02-18     
1 Bunge H J.Z Melallk,1965 56: 872
2 Roe R J.J Appl Phys,1965;36:2024
3 Morris P R, Heckler A J,Adv X-Ray Anal, 1968;11:454
4 徐家恢,梁志德,刘铸.东北工学院学报,1986;2:97
5 Liang Z D,Xu J Z,Wang F Texture Cryst Solids,1980 4: 93
6 梁志德,徐家桢,王福. 金属学报,1980;16:276
7 Zuo L,Zhao X,Xu J Z,Liang Z D.Textures Microstruct, 1988;10:59
8 Morris P R, Heckta A J. Trans Met Soc. AIME 1969; 245: 1987
9 Bunge H J.Mathematische Methoden der Texturanahae,Berlin:Akademle-Verlag,1969: 31
10 MorrisPR,Flowers J W.Texture Cryst Solids, 1981;4: 129
11 Morris P R,J Appl Phys, 1969; 40:447
12 王沿东,左良,徐家恢,梁志德, 电工钢,1989; 1-2: 71
13 Bunge H J, Roberts W T.J Appl Crystallogr, 1969; 2: 116
14 Matsuo M,Taut S, Kawasaki K.Proc ICOTOM6,Tokyo,1981:1250
15 Lucke K,Pospiech J, Virnich K H, Jura J. Acta Netakk, 1981;29:167
16 Matthies S. Phys STatus Solidi, 1979;B92:135
17 Liang Z D,Xu J Z, Wang F. Proc ICOTOM6, Tokyo, 1981;1259
18 Liang Z D,Xu J Z, Wang F.Mater Sci Eng,1983;60:59
19 Wanger F,Humbert M.Texlures Microstruct, 1987;7:115
20 Zhao X Zuo L,Liang Z D,Zhao H.Textures Microstruct, 1992 19: 63
21 Ruer D,Baro R. Adv X-Ray Anal, 1977; 20:187
22 Ruer D, Baro R.J Appl Crystallogr, 1977; 10: 4
23 Vadon A, Ruer D. Baro R.Proc ICOTOM6. Tokyo, 1981;1310
24 Ruer D,Vadon A,Baro R.Adv X-Ray Anal,1979;23:349
25 左良,徐家桢,梁志德. 中国科学, 1990: A(11):1217
26 Zuo L,Xu J Z, Liang Z D,J Appl Phys, 1989; 66:2338
27 左良,王沿东,徐家桢,梁志德. 金属学报,1989; 25:B215
28 Matthies S. Krist Tech,1980; 15:135
29 Bunge H J,Esling C.J Appl Crystallogr, 1981;14:253
30 Hjelen J, Qvale A M, Gomo O. Proc ICOTOMIO,Clausthal, 1993:137
31 Bunge H J,Esling C. Proc ICOTOM6、Tokyo, 1981:1210
32 Pospiech J, Lucke K, Jura J. Proc ICOTOM6,Tokyo, 1981:1390
33 Jaynes E T. Phys Rev, 1957; 106: 620
34 Wang F,Xu J Z, Liang Z D, Liang Z D. Proc ICOTOM8. Santa, 1987: 111
35 Wang F,Xu J Z, Liang Z D.Textures Microstruct, 1989 10: 217
36 Wang F,Xu J Z,Liang Z D.Textures Microstruct, 1992:19:55
37 Wang F,Xu J Z,Liang Z D.J Appl Crystallogr, 1991:24: 126
38 王沿东,徐家帧金属学报,1995; 31:B550
39 Wang Y D,Xu J Z.Scr Metall Mater, 1995; 33:1049
40 Jiang J X, Wang F, Liu Y S.Liang Z D. Proc ICOTOMII, Xi’an、1996: 112
41 Wang Y D, Xu J Z、Liang Z D.Textures Microstruct, 1995; 26-27;103
42 Wang Y D,Xu J Z,Zuo L,Liang Z D、Vadon A-Bessieres. Heizmann J J.Proc ICOTOMII,Xi’an.1996:1064
43 Wang Y D, Liu Y D, Xu J Z, Liang Z D,J Appl Phys, 1996; 79:7376
44 Wang Y D, Vadon A Heizmann J J. Xu J Z Scr Metall Mater, 1996:35:905
[1] 王沿东; 佟伟平; 何长树; 左良; 梁志德 . 含磷深冲钢板的低分辨织构分析与弹性模量预估[J]. 金属学报, 1999, 35(6): 627-630 .
[2] 王沿东;徐家桢. 具有重叠衍射峰低对称晶系材料的定量织构分析[J]. 金属学报, 1995, 31(24): 550-554.