| Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9合金的热磁分析 |
| 王治;何开元;张洛 |
| 东北大学;沈阳;110006;天津理工学院;天津;300191;东北大学;沈阳;110006;上海钢铁研究所;上海;200940 |
|
| MAGNETOTHERMAL ANALYSIS OF Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9 ALLOY |
| WANG Zhi;HE Kaiyuan;ZHANG Luo (Northeastern University; Shenyang 110006)(Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940) |
引用本文:
王治;何开元;张洛. Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9合金的热磁分析[J]. 金属学报, 1997, 33(12): 1289-1294.
,
,
.
MAGNETOTHERMAL ANALYSIS OF Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9 ALLOY[J]. Acta Metall Sin, 1997, 33(12): 1289-1294.
1Yoshizawa Y,Oguma S,Yamauchi K.J Appl Phys,1988;64:6044 2张延忠,年素珍,金惠娟,许桂琴,杨燮龙,李香箐.金属学报, 1995; 31: B212 3Wang Zhi,He Kaiyuan,He Shuli,Zhang Luo,Yin Jun,Zhang Yumei,Cheng Lizhi.Proceeding ofthe Ninth International Conference on Rapidly Quenched Materlals and MetastableAlloys, Bratislava, 1996 4Narita K, Yamasaki J, Fukunaga H. IEEE Trans Magn, 1980; 16: 4355 5Herzer G.IEEE Trans Magn,1989;25:3327 6He Kaiyuan, Zhou Fei, Zhi Jing, Cheng Lizhi. In: Kim C S, Lee T D, Oh J H eds.. Proceedings ofthe Third International Symposium on Physics of Magnetic Materials, Seoul, Korea: The KoreanMagnetics Society, 1995: 245 7Bozorth R M. Ferromagnetism. New York: Van Norstrand, 1951: 74 8Tebble R S, Craik D J. Magnetic Mater, 1969: 106 9oshizawa Y,Yamauchi K.Mater Sci Eng,1991;133:176 10Hasegawa R,Ray R.J Apppl Phys,1979;50:1586 11Herzer G.Mater Sci Eng,1991;133:1 12王治,何开元,贺淑莉,张玉梅,傅玉君,张洛.物理学报,1997; 46(6):134 |
|