| L1_2结构Ni_(74.5)Pd_2Al_(23.5)合金的反相畴界能 |
| 孙坚;李振声;赖其略 |
| 上海交通大学国家教委高温材料及高温测试开放实验室;上海;200030;香港城市大学;香港;香港城市大学;香港 |
|
| THE APB ENERGIES OF Ni_(74.5)Pd_2Al_(23.5) ALLOY WITH L1_2 STRUCTURE |
| SUN Jian(The Public Laboratory of State Education Commission.for High Temperature Materials and High Temperature Tests;Shanghai Jiaotong University; Shanghai 200030); C. S. Lee; J. K. L. Lai(City University of Hong Kong; Hong Kong) |
引用本文:
孙坚;李振声;赖其略. L1_2结构Ni_(74.5)Pd_2Al_(23.5)合金的反相畴界能[J]. 金属学报, 1997, 33(11): 1130-1134.
,
,
.
THE APB ENERGIES OF Ni_(74.5)Pd_2Al_(23.5) ALLOY WITH L1_2 STRUCTURE[J]. Acta Metall Sin, 1997, 33(11): 1130-1134.
1ChibaA,HanadaS,WatanbeS.MaterTransJIM,1991;39:824 2ChibaA,HanadaS,WatanbeS.BullJpnInstMet,1991;30:12 3KearBH,WilsdorfHG.TransMetallSocAIME,1962;224:382 4HirthJP,LotheJ.TheoryofDislocations.2nded,NewYork:John-Wiley&Sons,1982:423 5YooMN.ActaMetall,1987;35:1559 6DimidukDM,ThompsonAW,WilliamsJC.PhilosMag,1993;A67:675_ |
|