| 高技术时代的钛合金材料技术发展战略及对策剖析 |
| 张力 |
| 中国科学院应用研究与发展局;北京;100864 |
|
| AN ANALYSIS OF DEVELOPING STRATEGIES AND MEASURES OF TITANIUM BASED MATERIALS IN THE HIGH-TECHNOLOGY ERA |
| ZHANG Li (Bureau of Applied Research and Development; Chinese Academy of Sciences; Beijing 100864) |
引用本文:
张力. 高技术时代的钛合金材料技术发展战略及对策剖析[J]. 金属学报, 1997, 33(1): 85-89.
.
AN ANALYSIS OF DEVELOPING STRATEGIES AND MEASURES OF TITANIUM BASED MATERIALS IN THE HIGH-TECHNOLOGY ERA[J]. Acta Metall Sin, 1997, 33(1): 85-89.
|