Please wait a minute...
金属学报  1996, Vol. 32 Issue (8): 857-861    
  论文 本期目录 | 过刊浏览 |
气体雾化贮氢电极合金Ml(Ni,Co,Mn,Ti)_5的活化性能
周煜;雷永泉;罗永春;成少安;王启东;张永昌
北京大学;浙江大学;中国科学院金属研究所
ACTIVATION OF HYDROGEN-STORAGE ELECTRODE ALLOY Ml(Ni,Co,Mn,Ti)_5 PRODUCED BY GAS ATOMIZATION
ZHOU Yu(Peking University; Beijing 100871); LEI Yongquan; LUO Yongchun;CHENG Shao'an; WANG Qidong (Zhejiang University; Hangzhou 310027);ZHANG Yongchang (Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015) (Manuscript received 1995-09-24; in revised form 1996-04-14)
引用本文:

周煜;雷永泉;罗永春;成少安;王启东;张永昌. 气体雾化贮氢电极合金Ml(Ni,Co,Mn,Ti)_5的活化性能[J]. 金属学报, 1996, 32(8): 857-861.
, , , , , . ACTIVATION OF HYDROGEN-STORAGE ELECTRODE ALLOY Ml(Ni,Co,Mn,Ti)_5 PRODUCED BY GAS ATOMIZATION[J]. Acta Metall Sin, 1996, 32(8): 857-861.

全文: PDF(337 KB)  
摘要: 研究了感应熔炼后随炉冷却和经不同处理的气体雾化贮氢电极合金Ml(Ni,Co,Mn,Ti)_5的电化学活化特性.结果表明,氢化前后合金内能的变化是影响活化性能的原因.因表面覆盖氧化膜或任何其它原因所引起的附加内能越大,或氢化时氢原子进入四面体或八面体间隙位置所引起的应变能越大,活化越困难.
关键词 : 贮氢电极合金,  超声气体雾化,  电化学活化    
Abstract:The electrochemical activation behaviours of the hydrogenstorage electrode alloys Ml(Ni,Co,Mn,Ti)5 produced by induction melting and then fornace cooling (FC) or Ar-gas atomizing (AGA) have been studied by comparing the activation of AGA electrodes aged at room temperature for 4 months with that of FC electrode. It is found that the surface oxide is only a minor factor to affect the activation, while the magnitude of internal energy change in the alloy before and after hydrogenation is the controlling factor. The increases in the internal energy of the alloy, caused by oxide and the H-atoms entering tetrahedral or octahedral sites during hydrogenation, make the activation difficult. Correspondent:(ZHOU Yu, postdoctor, Department of Chemistry, Peking University, Beijing 100871)
Key words: hydrogen-storage electrode alloy    ultrasonic gas atomization    electrochemical activation
收稿日期: 1996-08-18     
1WallaceWE,KarllcekRF.JPhysChem,1979,83:17082PickMA,WenzlH.IntJHydrogenEnergy,1977;1:4133SchoberT.JLess-CommonMet,1983;89:634RudmanPS.JLess-CommonMet,1983;89:935ManchesterFD,KhatamianD.MaterSciForum,1988;31:2616LeiYongquan.JLess-CommonMet,1991;172:12657王云.中南矿冶学院学报,1991;22:178戴圣龙,于桂复,颜鸣皋.航空学报,1994;15:6969SinhaVK,WallaceWE.JLess-CommonMet,1983;91:239"
[1] 朱光明; 雷永泉; 陈立新 . 二元稀土系AB5型贮氢电极合金的放电容量与晶胞体积和4f电子的关系[J]. 金属学报, 2003, 39(7): 781-784 .
[2] 朱光明; 陈立新; 雷永泉; 王启东; 尤金跨; 林祖赓 . RE(Ni,Co,Mn,Ti)5合金(RE=La,Ce,Pr,Nd) 的单胞体积对电化学性能的影响[J]. 金属学报, 2001, 37(1): 61-66 .
[3] 杨晓光;雷永泉;张文魁;朱光明;王启东. (Zr,Ti)(V,Mn,Pd,Ni,Fe)_2系贮氢电极合金的循环稳定性[J]. 金属学报, 1996, 32(8): 852-856.