| 20钢奥氏体氮碳共渗后淬火态与时效态的化合物层 |
| 戎咏华;王永瑞;王纪文;陈行康;胡赓祥 |
| 上海交通大学 |
|
| COMPOUND LAYER STRUCTURE OF NITROCARBURIZING 120 STEEL AETER QUENCHING AND AGING |
| RONG Yonghua; WANG Yongrui; WANG Jiwen; CHEN Xingkang; HU Gengxiang(Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1995-09-21) |
引用本文:
戎咏华;王永瑞;王纪文;陈行康;胡赓祥. 20钢奥氏体氮碳共渗后淬火态与时效态的化合物层[J]. 金属学报, 1996, 32(5): 462-468.
,
,
,
,
.
COMPOUND LAYER STRUCTURE OF NITROCARBURIZING 120 STEEL AETER QUENCHING AND AGING[J]. Acta Metall Sin, 1996, 32(5): 462-468.
| 1BellT,KinaliM,MunstermannG.HeatTreatMet,1987;2:472陈行康,朱文琴.金属热处理,1988;2:163陈行康,王永瑞,戎咏华.金属热处理学报,1992;13:54WangYongrui,RongYonghua,ChenXingkang,HuGengxiang.MaterCharact,1995;34:2145杨承岳.测试技术,1985;6:336桶谷繁雄.电子线回折金属炭化物研究.1971:2097JacKKH.ProcRSocLondon,1948;1A:1958戎咏华,王闽,王永瑞,陈行康.理化检验(物理分册),1993;29:5 |
|