| Al-Li单晶体锯齿流变的形态特征 |
| 田宝辉;张永刚;陈昌麒 |
| 北京航空航天大学 |
|
| MORPHOLOGY OF SERRATED FLOW OF AI-Li SINGLE CRYSTALS |
| TIAN Baohui; ZHANG Yonggang; CHEN Changqi(Beijing University ofAeronautics and Astronautics; Beijing 100083) (Manuscript received 1 995-05- 1 6; in revised form 1 995-08-25) |
引用本文:
田宝辉;张永刚;陈昌麒. Al-Li单晶体锯齿流变的形态特征[J]. 金属学报, 1996, 32(3): 249-253.
,
,
.
MORPHOLOGY OF SERRATED FLOW OF AI-Li SINGLE CRYSTALS[J]. Acta Metall Sin, 1996, 32(3): 249-253.
| 1KingJE,YouCY,KnottJF.ActaMetall,1981;29:15532SivakesavamO,SahaGG,RaghavaSrinirasaK.MalerSciTechnol,1988;4:5783DelafasseD,LapassetG,KubinLP.ScrMetallMater,1993;29:13794KumarS,PinkE.ScrMetallMater.1995;32:7495PinkE,GrinbergA.MaterSciTechnol,1981;51:16FujitaH,TabataT.ActaMetallMaler,1977;25:7937HuangJC,GrayGT.ScrMetallMaler.1990:26:858BrechetY,EstinY.ScrMetall,1994;31:185 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|