| Al-l8%Si过共晶合金熔体结构特征及磷的影响 |
| 桂满昌;宋广生;贾均;李庆春 |
| 哈尔滨工业大学;北京航空材料研究所2室 |
|
| STRUCTURE OF MOLTEN HYPEREUTECTIC Al-18%Si ALLOY AND INFLUENCE OF PHOSPHORUS |
| GUI Manchang; SONG Guangsheng;JIA Jun; LI Qingchun(Harbin Institute of Technology;Hurbin 150001) |
引用本文:
桂满昌;宋广生;贾均;李庆春. Al-l8%Si过共晶合金熔体结构特征及磷的影响[J]. 金属学报, 1995, 31(4): 177-182.
,
,
,
.
STRUCTURE OF MOLTEN HYPEREUTECTIC Al-18%Si ALLOY AND INFLUENCE OF PHOSPHORUS[J]. Acta Metall Sin, 1995, 31(4): 177-182.