摘要: 本文提出一种不含Si的镍基Ni-Cr-Co-B高温钎料.对一系列Ni-Cr-Co-B钎料的熔化特性、钎焊工艺性能、钎料组织以及钎焊接头的室温和高温强度、接头韧性进行了研究,并与标准镍基钎料BNi-1a和BNi-5进行了比较研究结果表明,Ni-Cr-Co-B钎料钎焊的高温合金接头的高温性能和韧性均超过标准镍基钎料.
关键词 : Ni-Cr-Co-B钎料,  高温钎焊,  机械性能    
Abstract:For improving the toughness and elevated temperature mechanical properties of brazed superalloy joints, the silicon-free Ni-CrCo-B brazing filler alloys have been developed. The microstructure, melting characteristics and brazing properties of a series of Ni-CrCo-B filler metals were investigated. Mechanical properties at room and elevated temperatures of superalloy joints brazed with the Ni-Cr-Co-B filler metals were evaluated and compared with those of brazed joints with conventional nickel-base filler metals BNi-1a and BNi-5. It was shown that the toughness and high-temperature mechanical properties of the brazed joints made with the developed Ni-Cr-Co-B filler alloys are better than the latter.
Key words: brazing filler metal    high temperature brazing    mechanical propertiy
    
1KX著,金钦乾,徐澄宇,马翔译.钢和合金的物理化学相分析.北京:国防工业出版社,1982:1842LugscheiderE,PartzK-D.WeldJ,1983;62:160s
[1] 杨超, 卢海洲, 马宏伟, 蔡潍锶. 选区激光熔化NiTi形状记忆合金研究进展[J]. 金属学报, 2023, 59(1): 55-74.
[2] 罗 键 王向杰 赵国际 王家序. CO2+电磁搅拌复合堆焊梯度功能层的微观组织及性能研究[J]. 金属学报, 2009, 45(12): 1487-1492.
[3] 袁广银; 尹健; 丁文江 . Mg--Cu--Ni--Gd非晶合金结构弛豫及力学性能[J]. 金属学报, 2008, 44(2): 222-226 .
[4] 张毅; 周延春 . Ti3SiC2弥散强化Cu:一种新的弥散强化铜合金[J]. 金属学报, 2000, 36(6): 662-666 .
[5] 耿洪滨;何世禹;雷廷权. 热循环对TC4钛合金组织和机械性能的影响[J]. 金属学报, 1996, 32(1): 51-56.
[6] 刘向宏;吴晓祖;陈贞国;吴燧华. 界面扩散对316L-20钢复合线机械性能的影响[J]. 金属学报, 1993, 29(7): 40-43.