| CO还原CaO-SiO_2-Al_2O_3-Fe_tO渣系研究 |
| 杨学民;郭占成;于宪溥;艾菁;王大光 |
| 中国科学院化工冶金研究所 |
|
| REDUCTION OF CaO-SiO_2-Al_2O_3-Fe_ tO QUARTERNARY SLAG SYSTEM BY CO |
| YANG Xuemin; GUO Zhancheng; YU Xianpu; AI Jing; WANG Daguang (Institute of Chemical Metallurgy; Chinese Academy of Sciences; Beijing)(Manuscript received 25 March;1994) |
引用本文:
杨学民;郭占成;于宪溥;艾菁;王大光. CO还原CaO-SiO_2-Al_2O_3-Fe_tO渣系研究[J]. 金属学报, 1994, 30(23): 491-498.
,
,
,
,
.
REDUCTION OF CaO-SiO_2-Al_2O_3-Fe_ tO QUARTERNARY SLAG SYSTEM BY CO[J]. Acta Metall Sin, 1994, 30(23): 491-498.
| 1NagaskaT,IguchiY,Ban-yaS.FifthInternationalIronandSteelCong.April6-9,l986,WashingtonDC,USA,6692FineH,MeyerD,JankeD,EngelH-J.IronmakingSteelmaking,1985,12(4):1573杨学民,王大光,宣德茂,唐武成,第八届冶金物理化学学术研讨会论文集,苏州,1992:1534杨学民,王大光,刘天中,宣德茂,唐武成.化工冶金,1994:15:75杨学民,王大光,宣德茂,唐武成.化工冶金,1993;14:1956杨学民,王大光,宣德茂,唐武成,化工冶金,1995;16:77杨学民,王大光,宣德茂.金属学报,1993;29:B3418DuffyJA,IngramMD.JAmChemSoc.,1991;93:64489YoungRW,DuffyJA,HassallGJ,XuZ..IronmakingSteelmakig,1992;19:20110BergmanA.SteelRes,1990;61:34711GaskellDR.TransISIJ,1982;22:99712NagabayashiR,HinoM,Ban-yaS.ISIJInt,1989;29:14013Ban-yaS.ISIJInt,1993;33:214万谷志郎,日野光兀,汤下宪志,铁钢,1985;71:85315万谷志郎,日野光兀,竹添英孝.铁钢,1985;71:190316Ban-yaS,HinoM.ChemicalPropertiesofMoltenSlags.Tokyo:TheIronandSteelInstituteofJapan,1991:275 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|