Please wait a minute...
金属学报  1994, Vol. 30 Issue (10): 463-468    
  论文 本期目录 | 过刊浏览 |
Ti-1023合金拉伸试验的电镜原位观察
朱维斗;顾海澄;郭延东
西安交通大学;西安交通大学材料系
IN SITU TENSION OBSERVATION ON Ti-10V-2Fe-3Al ALLOY UNDER SEM AND TEM
ZHU Weidou;GU Haicheng; GUO Yandong(Xi′an Jiaotong University)(Manuscript received 7 December; 1993; in revised form 14 March; 1994)
引用本文:

朱维斗;顾海澄;郭延东. Ti-1023合金拉伸试验的电镜原位观察[J]. 金属学报, 1994, 30(10): 463-468.
, , . IN SITU TENSION OBSERVATION ON Ti-10V-2Fe-3Al ALLOY UNDER SEM AND TEM[J]. Acta Metall Sin, 1994, 30(10): 463-468.

全文: PDF(512 KB)  
摘要: 用扫描电镜和透射电镜原位观测了Ti-10V-2Fe-3Al合金经固溶处理获得亚稳定β相后在拉伸过程中α″相的形成、长大及裂纹的萌生与扩展,以及最终断裂过程.并采用DIC金相方法方便地区分滑移线和α″相.
关键词 : Ti-10V-2Fe-3Al,  原位拉伸观测    
Abstract:The in situ tension observations of SEM and TEM were carried out on specimens of a β solution treated Ti-10V-2Fe-3Al alloy with a sharp notch. Following tensile load increase the β→α″phase transformation and a″plate growth was clearly demonstrated.Owing to the SEM specimens were made of rather thin plates so the fracture was purely in ductile shear mode. The crack initiations took place on slip bands and the crack growth followed the re-nucleation and coalescence manner.DIC optical microscopy was used to identify the slip lines and a″plates.Correspondent: ZHU Weidou, associate professor, Department of Materials, Xi′an Jiaotong University, Xi′an710049
Key words: Ti-10V-2Fe-3Al    in situ tension observation
收稿日期: 1994-10-18     
基金资助:国家自然科学基金
1李青云.第六届全国钦及钛合金学术交流会文集(1),1987:12DueringTW,MiddletonRM,TerlindeGT,WilliamsJC.Titanium′80,V.2:15033宋书娟.西安交通大学硕士论文,19894JeffreyR,BiedrmanRR.Titanium′80,V.2:4915LiebowitzH.AnAdvancedTreatiseI.NewYork:AcademicPressInc,1968:3356BroekD.ElementaryEngineeringFractureMechanics,3rdreviseded,Hague:MartinusNijhoffPublishers,1983:38
[1] 杨蕊,潘艳,陈威,孙巧艳,肖林,孙军. 微尺度Ti-10V-2Fe-3Al单晶压缩变形行为及其微观机制*[J]. 金属学报, 2016, 52(2): 135-142.