Please wait a minute...
金属学报  1994, Vol. 30 Issue (1): 11-19    
  论文 本期目录 | 过刊浏览 |
一种含Nd耐热钛合金强化机制的研究
孙福生;曹春晓
北京航空材料研究所
STRENGTHENING BEHAVIOUR OF A HIGH-TEMPERATURE Ti ALLOY CONTAINING Nd
SUN Fusheng;CAO Chunxiao;(Beijing Institute of Aeronautical Materials)(Manuscript received 15 June;1993;in revised form 24 August;1993)
引用本文:

孙福生;曹春晓. 一种含Nd耐热钛合金强化机制的研究[J]. 金属学报, 1994, 30(1): 11-19.
, . STRENGTHENING BEHAVIOUR OF A HIGH-TEMPERATURE Ti ALLOY CONTAINING Nd[J]. Acta Metall Sin, 1994, 30(1): 11-19.

全文: PDF(608 KB)  
摘要: 研究了Nd对Ti-5.5Al-4.5Sn-2Zr-lMo-0.25Si-Nd耐热钛合金的组织、室温拉伸性能和热稳定性能的影响及其机.制结果表明,Nd可以细化组织,密化位错网亚晶界,改善室温拉伸强度和热稳定性能,Nd的强化机制主要由细晶强化(尤其是位错网亚晶界强化)和基体中Sn、O贫化引起的弱化的综合.
关键词 : 耐热钛合金,  强化机制.Nd    
Abstract:Influence of Nd on microstructure,tensile properties,thermal stability and strengthening behaviour of Ti-5.5A1-4.SSn-2Zr-1Mo-0.25Si-Nd alloy was studied,Nd can not only refine the prior β grains and α plates,and especially densify dislocation network subgrain boundaries,but also improves tensile strength and thermal-stability.The strengthening of Nd is superposition of strengthening caused by grain-refinement,particularily the densifying of subgrain boundaries,and weakening caused by depletion of Sn and O2 in matrix phase.Correspondent:SUN Fusheng,senior engineer.Laboratory No.15,(Beijing Institue of Aeronautical Materials,Beijing 100095)
Key words: TiAlSnZrMoSiNd alloy    strengthening    Nd
收稿日期: 1994-01-18     
1SastrySML,PengTC,O'NealJE,TitaniumScienceandTechnology,1984;l:3972SastrySML,MeschterPJ,O'NealJE,MetallTrans,1984;15A:14513KonitzerDG,MuddleBC,FraserHL,MetallTrans,1983;14A:19794KonitzerDG,ScriptaMetall,1983;17:9635WangSH,ProcMaterResSocSymp,1984;28:367 6Bowden DM,SastrySMLet.al,TitaniumSciTech,1984;2:7837李东,刘羽寅,钛科学与工程,1987;2:498杨冠军,韩传玺.钛科学与工程,1987;2:699秦蔡庆,唐仕生.钛科学与工程,1987;3:6310陈克修,罗月新.钛科学与工程,1987;2:4211金相实验技术,清华大学教学讲义,1983年10月12孙福生,硕士学位论文,北京航空材料研究所,1988年12月13孙福生,曹春晓.材料工程,1991;3:4814MottNF,NabarroFRN,ReportofConferenceonStrengthofSolids,194815EA著,陈石卿译.钛合金金相学,北京:国防工业出版社,198616王金友,葛志明,周彦邦.航空用钛合金,上海科学技术出版社,1985:6017张树文,李永森.钛科学与工程,1987;2:4418FleischerRL.ActaMet,1963;11:20319SastrySML,MetalTrans.1984;15A:146520FelthamP.JApplphys.1968;1:30321AssbyMF,In:KelleyA,etaleds.,StrenglheningMethodsinCrvstals,JohnWiley,NewYork,1971:137.
No related articles found!