一种低合金高强度钢中(Ti_xV_(1-x))(C_yN_(1-y)粒子对焊接热循环的响应
桂赤斌;崔昆
博士;武汉(430074);华中理工大学机械工程系;华中理工大学
RESPONSE OF (Ti_xV(1-x))(C_yN_(1-y)) PARTICLES IN HSLA STEEL TO WELD THERMAL CYCLES
GUI Chibin;CUI Kun Huazhong University of Science and Technology; Wuhandoctor;Department of 2nd Mechanical Engineering;Huazhong University of Science and Technollogy;Wuhan 430074
引用本文:

桂赤斌;崔昆. 一种低合金高强度钢中(Ti_xV_(1-x))(C_yN_(1-y)粒子对焊接热循环的响应[J]. 金属学报, 1993, 29(8): 77-80.
, . RESPONSE OF (Ti_xV(1-x))(C_yN_(1-y)) PARTICLES IN HSLA STEEL TO WELD THERMAL CYCLES[J]. Acta Metall Sin, 1993, 29(8): 77-80.

全文: PDF(478 KB)  
摘要: 研究了低合金高强度钢中(Ti_xV_(1-x))(C_yN_(1-y))粒子对焊接热循环的响应特性其表现是:(1)溶解滞后效应,(2)粗化速率非常缓慢
关键词 : 低合金高强度钢,  (Ti_xV_(1-x))(C_yN_(1-y))粒子,  焊接热循环    
Abstract:(Ti_xV_(1-x))(C_yN(1-y)) particles in HSLA steel, subjected to weld thermal cycles, wasobserved to lag behind in dissolution, which reduces with the increase of peak temperature.And the coarsening rate of these particles is very slow.
Key words: HSLA steel    (Ti_χV_(1-χ))(C_yN_(1-y))    particle    weld thermal cycle
收稿日期: 1993-08-18     
1 Ion J C, Easterling K E, Ashby M F. Acta Metall, 1984; 32: 1949
2 Ashby M F, Easterling K E. Acta Metall, 1982; 30: 1969
3 桂赤斌,崔昆,李志远.焊接学报,1990;11:136
4 McCutcheon D B, McGrath J T, Godden M J, Ruddle G E, Weatherly G, Houghton D C. ASTM STP 792, 1982: 227
5 Cuddy L J,Lally J S,Porter L F.高强度低合金钢工艺与应用国际会议论文集(中译本,第二分册),鞍山钢铁公司钢铁研究所,1986:326
6 Suzuki S, Weatherly G C, Houghton D C. Acta Metall, 1987; 35: 341
7 肖纪美著,合金热力学(下册),北京钢铁学院1982:94
8 Matsuta S, Okumura N, Trans. ISIJ, 1978; 18: 198
[1] 张苏强,赵洪运,舒凤远,王国栋,贺文雄. 焊接热循环对Q315NS钢在H2SO4溶液中腐蚀行为的影响[J]. 金属学报, 2017, 53(7): 808-816.
[2] 吴栋, 王鑫, 董文超, 陆善平. 焊接热循环及时效处理对一种Ni-Fe基高温合金的组织和力学性能的影响*[J]. 金属学报, 2014, 50(3): 313-322.
[3] 陈茂爱; 武传松; 杨敏; 唐逸民; 吴人洁 . Ti-V-Nb微合金钢第二相粒子在焊接热循环过程中的变化规律[J]. 金属学报, 2004, 40(2): 148-154 .
[4] 李亚江;邹增大;陈祝年;魏星;江全昌. 焊接热循环对HQ130钢热影响区组织及性能的影响[J]. 金属学报, 1996, 32(5): 532-537.