Please wait a minute...
金属学报  1993, Vol. 29 Issue (2): 70-73    
  论文 本期目录 | 过刊浏览 |
SmCl_3-PbCl_2和SmCl_3-PbCl_2-CaCl_2系相图的研究
王淑兰;张翊凤;隋殿鹏
东北工学院化学系;讲师;沈阳(110015);东北工学院;东北工学院
PHASE DIAGRAMS OF SmCl_3-PbCl_2 AND SmCl_3-PbCl_2-CaCl_2
WANG Shulan;ZHANG Yifeng;SUI Dianpeng Northeast University of Technology; Shenyang
引用本文:

王淑兰;张翊凤;隋殿鹏. SmCl_3-PbCl_2和SmCl_3-PbCl_2-CaCl_2系相图的研究[J]. 金属学报, 1993, 29(2): 70-73.
, , . PHASE DIAGRAMS OF SmCl_3-PbCl_2 AND SmCl_3-PbCl_2-CaCl_2[J]. Acta Metall Sin, 1993, 29(2): 70-73.

全文: PDF(287 KB)  
摘要: 利用DTA和X射线衍射技术研究了SmCl_3-PbCl_2二元系和SmCl_3-PbCl_2-CaCl_2三元系相图。发现SmCl_3-PbCl_2系有一个异份熔化化合物3SmCl_3 PbCl_2,体系转熔点p为465℃,42.0mol-%SmCl_3,低共熔点e是452℃,33.0mol-%SmCl_3,SmCl_3-PbCl_2-CaCl_2三元系有对应SmCl_3,PbCl_2,CaCl_2,和3SmCl_3·PbCl_2四个液相面,五条二次结晶线,一个三元低共熔点E[396℃,29.5mol-%SmCl_3,58.0mol-%PbCl_2],一个三元转熔点P[417℃,36.0mol-%SmCl_3,50.0mol-%PbCl_2),对应的两个四相平衡反应为: L=PbCl_2+CaCl_2+3SmCl_3·PbCl_2 L+SmCl_3=3SmCl_3·PbCl_2+CaCl_2
关键词 : SmCl_3-PbCl_2-CaCl_2三元系,  熔盐相图    
Abstract:Phase diagrams of binary system SmCl_3-PbCl_2 and ternary systemSmCl_3-PbCl_2-CaC_2, have been determined by DTA and X-ray diffraction analyses. In theSmCl_3-PbCl_2 system, an incongruent compound 3SmCl_3-PbCl_2, an eutectic point at 452℃containing 33.0 mol-% SmCl_3 and a peritectic point at 465℃ containing 42.0 mol-%SmCl_3 were obtained. In the SmCl_3-PbCl_2-CaCl_2 system, 4 liquiduses corresponding to theprimary crystallization of SmCl_3, PbCl_2, CaCl_2, and 3SmCl_3·PbCl_2, respectively, 5unvariant lines related to the secondary crystallization, a ternary eutectic point at 396℃ con-taining 29.5 SmCl_3 and 58.0 PbCl_2 by mol-% and a ternary peritectic point at 417℃ con-taining 36.0 SmCl_3 and 50.0 PbCl_2 by mol-% were found. Two reactions corresponding to 4phase equilibriums are L=CaCl_2+PbCl_2+3SmCl_3·PbCl_2 and L+SmCl_3=CaCl_2+3SmCl_3·PbCl_2.
Key words: phase diagram    SmCl_3    PbCl_2    CaCl_2
收稿日期: 1993-02-18     
1 张翊凤,孟波.金属学报,1991;27:B438
2#12 1970;43(8) :1835
3 Coleman D S, Long P D A. Trans Inst Min Metall, 1968; 77C: 170
4 苏勉曾,李根培.化学通报,1979;(4) :34
5 乔芝郁,王明生,郑朝贵,段淑贞.金属学报,1989;25:B234
6 郑朝贵,刘红平,乔芝郁,叶于浦.金属学报,1990;26:B68
[1] 许茜;于亚鑫;邱竹贤. LiF-CaF_2,NaF-CaF_2和KF-CaF_2系熔体热力学参量及相图的计算[J]. 金属学报, 1994, 30(16): 150-155.
[2] 唐波;钦佩;柳妙修;张未名;陈念贻. 人工神经网络在熔盐相图中间相预报中的应用[J]. 金属学报, 1994, 30(13): 22-26.
[3] 李瑞青;周国治. NaCl-BaCl_2-SrCl_2三元熔盐相图的计算[J]. 金属学报, 1989, 25(3): 90-95.