| 16Mn钢疲劳短裂纹扩展 |
| 王维明;黄雨华;徐灏 |
| 东北工学院;博士生;沈阳(110006)东北工学院175信箱;东北工学院;东北工学院 |
|
| PROPAGATION OF FATIGUE SHORT CRACKS IN STEEL 16Mn |
| WANG Weiming; HUANG Yuhua; XU Hao (Northeast University of Technology; Shenyang) |
引用本文:
王维明;黄雨华;徐灏. 16Mn钢疲劳短裂纹扩展[J]. 金属学报, 1992, 28(9): 42-46.
,
,
.
PROPAGATION OF FATIGUE SHORT CRACKS IN STEEL 16Mn[J]. Acta Metall Sin, 1992, 28(9): 42-46.
1 Pearson, S. Eng Fract Mech, 1975; 7: 235 2 Leis N B, Forts T P. ASTM STP 743, 1981: 100 3 Harada S, Murakami Y, Fukushima Y, Endo T. ASTM STP 942, 1988:1181 4 El Haddad M H, Smith K N, Topper P N. J Eng Mater Technol, 1979; 101: 42 5 Nisitani H. In: Tanaka T, Joho M, Komai K eds., Current Research on Fatigue Cracks, Kyoto: The Socisty of Materials Science Japan, 1985:1a |
|