| Fe-Mn-Al三元相图1000和1100℃等温截面的研究 |
| 刘兴军;郝士明;孙荣耀 |
| 东北工学院材料科学与工程系;沈阳110006;东北工学院;东北工学院 |
|
| ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM |
| LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang) |
引用本文:
刘兴军;郝士明;孙荣耀. Fe-Mn-Al三元相图1000和1100℃等温截面的研究[J]. 金属学报, 1992, 28(7): 50-54.
,
,
.
ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM[J]. Acta Metall Sin, 1992, 28(7): 50-54.
1 Banerji S. Adv Met Prog, 1987; 4: 59 2 Charles J, Berghezan A, Lutts A, Dancoisne P L. Met Prog, 1981; 119(6) : 71 3 张彦生.金属学报,1986;22:A470 4 Schmatz D J. Trans AIME, 1959; 215: 112 5 Chakrabarti D J. Metall Trans, 1977; 8B: 121 6 郝士明,刘兴军.中国物理学会第五届全国相图会议文集,武汉,1988) |
|