| 接触疲劳过程中的诱发相变和冷作硬化 |
| 张同俊;胡镇华;沈关学;崔崑 |
| 华中理工大学机二系金属材料教研室;副教授武汉(430074);华中理工大学;华中理工大学;华中理工大学 |
|
| INDUCED TRANSFORMATION AND COLD WORKED HARDENING IN THREE STEELS DURING CONTACT FATIGUE |
| ZHANG Tongjun;HU Zhenhua;SHEN Guanxue;CUI Kun Huazhong University of Science and Technology; Wuhan |
引用本文:
张同俊;胡镇华;沈关学;崔崑. 接触疲劳过程中的诱发相变和冷作硬化[J]. 金属学报, 1991, 27(2): 66-70.
,
,
,
.
INDUCED TRANSFORMATION AND COLD WORKED HARDENING IN THREE STEELS DURING CONTACT FATIGUE[J]. Acta Metall Sin, 1991, 27(2): 66-70.
1 Zackay V F, Parker E R, Fahr D, Busch R. ASM Trans Q, 1967; 60: 252 2 姜秉元,邵尔玉,金属学报,1986;22: A297 3 Chen H C, Era H, Shimizu M. Metall Trans, 1989; 20A: 437 4 Fultz B, Morris J W Jr. Metall Trans, 1985; 16A: 173 5 Moore M A, Richardson R C D, Attwood D G. Metall Trans, 1972; 3: 2485 6 Snell E O, Shyne J C, Goldberg A. Metallography, 1977; 10: 299 7 Habig K H 著,严立译.材料的磨损与硬度,北京:机械工业出版社,1987:274 8 Zhang Tongjun. Hu Zhenhua, Shen Guanxue. Cui Kun. On the Contact Fatigue in Leading Screw Steel for Precise Ball Bearing, C-MRS-Internation'90 Symposium, June 18-22, 1990 9 吴家龙·弹性力学·上海:同济大学出版社,1987:320 10 Fujita K, Yoshida A. Wear, 1979; 52: 37 11 Leng Xiaogang, Chen Qing, Shao Eryu. Wear. 1988; 122: 33Y |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|