| 超纯奥氏体不锈钢00Cr25Ni22Mo_2N非敏化态晶间腐蚀与磷(硅)的晶界偏聚 |
| 方耀华;徐源;张文奇 |
| 南京化工学院应用化学系;副教授;南京(210009);北京科技大学;北京科技大学 |
|
| INTERGRANULAR CORROSION AND PHOSPHOR SEGREGATION AT GRAIN BOUNDARY OF NON-SENSITIZED 00Cr25Ni22Mo2N SUPERPURE AUSTENITIC STAINLESS STEEL |
| FANG Yaohua;XU Yuan;ZHANG Wenqi Nanjing Institute of Chemical Technology University of Science and Technology Beijing FANG Yaohua; associate professor; Deportment of Applied Chemistry; Nanjing Institute of Chemical Technology; Nanjing 210009 |
引用本文:
方耀华;徐源;张文奇. 超纯奥氏体不锈钢00Cr25Ni22Mo_2N非敏化态晶间腐蚀与磷(硅)的晶界偏聚[J]. 金属学报, 1989, 25(6): 91-95.
,
,
.
INTERGRANULAR CORROSION AND PHOSPHOR SEGREGATION AT GRAIN BOUNDARY OF NON-SENSITIZED 00Cr25Ni22Mo2N SUPERPURE AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 1989, 25(6): 91-95.
1 Armijo J S. Corrosion, 1968; 24: 24 2 Aust K T. TMS-AIME, 1969; 245; 2117 3 Joshi A, Stein D F. Corrosion, 1972; 28: 321 4 Briant G J. Corrosion, 1980; 36: 508 |
|