Please wait a minute...
金属学报  1989, Vol. 25 Issue (5): 72-75    
  论文 本期目录 | 过刊浏览 |
热浸Al-Si渗层的组织分析
李翠屏;刘兴志;田继丰;高允彦
中国科学院金属研究所;工程师;沈阳(110015);中国科学院金属研究所;中国科学院金属研究所;东北工学院
STRUCTURE ANALYSIS OF HOT IMPREGNATED Al-Si COATING
LI Cuiping;LIU Xingzhi;TIAN Jifeng;GAO Yunyan Institute of Metal Research; Academia Sinica; Shenyang Northeast University of Technology; Shenyang LI Cuiping; Institute of Metal Research; Academia Sinica; 110015 Shenyang
引用本文:

李翠屏;刘兴志;田继丰;高允彦. 热浸Al-Si渗层的组织分析[J]. 金属学报, 1989, 25(5): 72-75.
, , , . STRUCTURE ANALYSIS OF HOT IMPREGNATED Al-Si COATING[J]. Acta Metall Sin, 1989, 25(5): 72-75.

全文: PDF(977 KB)  
摘要: 用扫描电镜、电子探针和X射线衍射方法对热浸Al-Si渗层的组织进行了化学成分和结构分析,探讨了形成机制。
关键词 : 热浸渗铝,  渗层结构分析 Al-Si渗层    
Abstract:The microstructure and chemical composition of the hot impregnated Al-Si coat-ing on 08Al steel sheet were analysed by SEM, EPMA and X-ray diffraction. The coatingis xonstitated by three parts: the outer is an α-Al solid solution of enriched Si and γ- (Fe,Al, Si) phases; the intermediate FeAl_3 and Fe_2Al_5 phases mainly and the inner neighbouringupon the substrate mainly Fe_2Al_5 phase.
Key words: impregnating coating    structure analysis    Al-Si impregnation
收稿日期: 1989-05-18     
1 Buehler H E. Prakt Metallogr, 1977; 14: 341--362
2 Coburn K G. Metallurgia, 1959; 60 (357) : 17--20
3 内田幸夫,藤田充,広濑祐辅.金属表面技术,1982;33:537--543
4 Larikov L N, Fal'chenko V M, Polishchuk D F, Ryabov V R, Lozovskaya A V. In: Samsonov G V ed, Protective Coatings on Metals, Vol. Ⅲ, New York: Consultants Bureau, 1971: 66--70
5 Willey L A. Metals Hand Book, Vol. Ⅷ, 8th ed, Metals Park, Ohio: ASM, 1973: 394--395
6 平野贤一,菱沼章道.日本金属学会志,1968;32:516--521
7 Ryabov V R. In: Samsonov G V ed, Protective Coatings on Metals, Vol. Ⅲ, New York: Consultants Bureau, 1971; 96--100
8 江岛辰彦,山村力,内田直人,松琦温,二阶堂胜.日本金属学会志,1980;55:316--32
No related articles found!