金属学报  1989, Vol. 25 Issue (2): 95-99    
  论文 本期目录 | 过刊浏览 |
定向反应合成高T_C超导化合物YBa_2Cu_3O_x
樊占国;冀春霖;王魁汉;崔传孟;刘素兰
东北工学院;东北工学院冶金物化教研室;教授;沈阳;东北工学院;东北工学院;东北工学院
HIGH T_c SUPERCONDUCTOR YBa_2 Cu_3 O_x PREPARED WITH DIRECT REACTION PROCESS
FAN Zhanguo;JI Chunlin;WANG Kuihan;CUI Chuanmeng;LIU Sulan Northeast University of Technology; Shenyang
引用本文:

樊占国;冀春霖;王魁汉;崔传孟;刘素兰. 定向反应合成高T_C超导化合物YBa_2Cu_3O_x[J]. 金属学报, 1989, 25(2): 95-99.
, , , , . HIGH T_c SUPERCONDUCTOR YBa_2 Cu_3 O_x PREPARED WITH DIRECT REACTION PROCESS[J]. Acta Metall Sin, 1989, 25(2): 95-99.

全文: PDF(371 KB)  
摘要: 提出定向反应合成过程制备液氮温区超导化合物YBa_2Cu_3O_x;报道了制备零电阻温度为90—94.5K,ΔT=1K的YBa_2Cu_3O_x的试验结果;试验确定并讨论了Y_2Cu_2O_5-CuO-YBa_2Cu_3O_(6.5)-Y_2BaCuO_5区域内的相平衡关系。
关键词 定向反应合成YBa_2Cu_3O_x高T_C超导体    
Abstract:A direct reaction process for producing high T_c spuerconductor YBa_2-Cu_3O_x has been proposed. The T_c of it is 90--94.5 K and △T is 1K. The phaseequilibria in system Y_2 BaCuO_5-Y_2Cu_2O_5-CuO-YBa_2Cu_3O_x were studied and discussed.
Key wordsdirect reaction process    YBa_2Cu_3Ox    high T_c superconductor
收稿日期: 1989-02-18     
1 Frase K G, Liniger E G, Clarke D R. J Am Ceram Soc, 1987; 70 (9) : C204
2 Che Guangcan (车广灿), Liang Jingkui (梁敬魁), Chen Wei (陈维) et al. Int J Mod Phys, B, 1987; 1 (2) : 363
No related articles found!