Please wait a minute...
金属学报  1988, Vol. 24 Issue (2): 194-198    
  论文 本期目录 | 过刊浏览 |
用TiFe_(0.86)Mn_(0.1)合金分离氢中Kr,Xe的研究
杨民杰;陈炳兆
中国科学院上海冶金研究所;中国科学院上海冶金研究所
SEPARATION AND CONCENTRATION OF Kr AND Xe FROM HYDROGEN USING TiFe_(0.86)Mn_(0.1) ALLOY
YANG Minjie;CHEN Bingzhao Shanghai Institute of Metallurgy; Academia Sinica
引用本文:

杨民杰;陈炳兆. 用TiFe_(0.86)Mn_(0.1)合金分离氢中Kr,Xe的研究[J]. 金属学报, 1988, 24(2): 194-198.
, . SEPARATION AND CONCENTRATION OF Kr AND Xe FROM HYDROGEN USING TiFe_(0.86)Mn_(0.1) ALLOY[J]. Acta Metall Sin, 1988, 24(2): 194-198.

全文: PDF(321 KB)  
摘要: 本文叙述用TiFe_(0.86)Mn_(0.1)合金作分离材料,分离、浓缩氢中Kr,Xe的基本原理和在不同温度下氢中Kr,Xe的分离情况.实验证明在300K时氢中Kr,Xe的分离浓度和放氢量的关系符合N=ae~(-bV)方程(N—浓度).
关键词 钛铁锰合金储氢性能    
Abstract:Separation and concentration processes of Kr and Xe from hydrogenusing TiFe_(0.86)Mn_(0.1) alloy have been investigated at different temperatures. The resultsshow that the relation betwecn the concentration of Kr and Xe and the amountof desorpted hydrogen at 300 K obeys the equation N=αe~(-bV).
Key wordsTi-Fe-Mn alloy    Kr    Xe    hydrogen storage property
收稿日期: 1988-02-18     
1 中国科学院上海冶金研究所.3. 5M~3储氢合金瓶的特性及其使用说明,1983
2 Wenzl H. Int Metall Rev, 1982. 17(3) : 140
3 Shinjiro Wakao. Function and Materials. 1983; 3(4) : 1
4 复旦大学化学系.物理化学下册,1978;187
5 桂光燕,傅继文.特种气体,1985;2:51
[1] 李谦, 孙璇, 罗群, 刘斌, 吴成章, 潘复生. 镁基材料中储氢相及其界面与储氢性能的调控[J]. 金属学报, 2023, 59(3): 349-370.
[2] 黄鹤飞, 李健健, 刘仁多, 陈怀灿, 闫隆. 316奥氏体不锈钢离子辐照损伤中的温度效应研究[J]. 金属学报, 2014, 50(10): 1189-1194.
[3] 汪洋; 张琰; 王新华; 陈长聘 . Ti-Cr基合金的储氢性能及晶体结构[J]. 金属学报, 2006, 42(6): 641-646 .
[4] 吕光烈; 舒康颖; 胡秀荣; 顾建明; 宋雪雁; 雷永泉; 王启东 . 快凝合金Zr(Ni0.55Mn0.3V0.1Cr0.05)2.1的相结构与储氢性能[J]. 金属学报, 1999, 35(5): 453-457 .
[5] 敖鸣;王启东. 经四氢呋喃改性后Mg的储氢性能[J]. 金属学报, 1990, 26(3): 40-43.