| Co-Er准晶态合金研究 |
| 李华;姜寿亭;丘梅影;郭贻诚;R.C.O’HANDLEY |
| 山东大学物理系;讲师;山东大学物理系;山东大学物理系;山东大学物理系;美国麻省理工学院 |
|
| QUASICRYSTAL Co-Er ALLOYS |
| LI Hua Department of Physics;Shandong University;Jinan;JIANG Shouting;QIU Meiying;GUO Yicheng;O'Handley R. C. Department of Physics; Shandong University; Jinan Massachussetts Institute of Technology; Cambridge |
引用本文:
李华;姜寿亭;丘梅影;郭贻诚;R.C.O’HANDLEY. Co-Er准晶态合金研究[J]. 金属学报, 1988, 24(2): 131-134.
,
,
,
,
.
QUASICRYSTAL Co-Er ALLOYS[J]. Acta Metall Sin, 1988, 24(2): 131-134.
1 Shechtman D S, Blech I, Gratias D, Cahn J W. Phys Rev Lett, 1984; 53: 1951 2 Steinhardt P H, Nelson D R, Ronchetti M. Phys Rev B, 1984; 28: 784 3 Steinhardt P J, Levine D., Phys Rev Lett, 1984; 53: 2477 4 Penrose R. Scientific American, 1977; (1) : Mathematical Games column S Lilienfeld D A, Nasfasi M, Johnson H H, Ast D G, Mater J W. Phys Rev Lett, 1985; 55: 1587 6 McHenry M E, Eberhart M E, O' Handley R C, Johnson K H. Phys Rev Lett, 1986; 56: 81 7 Jouve H, Roubillat J P, Meyer R. AIP Conf Proc, 1976; 29: 97 8 Buschow K H J, Fast J F, Van der Groot A S. Phys State Solid, 1968; 29: 825 9 Coey J M D. J Appl Phys, 1978; 49(3) : 164 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|