| 低碳Mn-Nb-V和Mn-Mo-Nb-V钢中的贝氏体转变 |
| 曹仁焕;马洪悌;阎振棨 |
| 东北工学院;东北工学院;东北工学院金属材料系;教授;沈阳文化路 |
|
| BAINITIC TRANSFORMATION IN LOW CARBON Mn-Nb-V AND Mn-Mo-Nb-V STEELS |
| CAO Renhuan;MA Hongti Northest University of Technology;ShenyangYAN Zhenqi Professor;Depariment of Metallic Materials;Northeast University of Technology;Wenhua Rood;Shenyang |
引用本文:
曹仁焕;马洪悌;阎振棨. 低碳Mn-Nb-V和Mn-Mo-Nb-V钢中的贝氏体转变[J]. 金属学报, 1988, 24(2): 135-138.
,
,
.
BAINITIC TRANSFORMATION IN LOW CARBON Mn-Nb-V AND Mn-Mo-Nb-V STEELS[J]. Acta Metall Sin, 1988, 24(2): 135-138.