| Cu-Zn-Al记忆合金稳定化过程的研究 |
| 谭树松;高秀娟 |
| 中南工业大学;中南工业大学 |
|
| DYNAMIC PROCESS OF MARTENSITIC STABILIZATION IN A Cu-Zn-Al ALLOY |
| by TAN Shusong; GAO Xiujuan (South-Central Polytechnic University) (Manuscript received 28 October; 1985; revised manuscript 18 July; 1986) |
引用本文:
谭树松;高秀娟. Cu-Zn-Al记忆合金稳定化过程的研究[J]. 金属学报, 1987, 23(6): 527-530.
,
.
DYNAMIC PROCESS OF MARTENSITIC STABILIZATION IN A Cu-Zn-Al ALLOY[J]. Acta Metall Sin, 1987, 23(6): 527-530.
1 谭树松,黄健超.中南矿冶学院学报,1984;(4) :19 2 祝向永,唐远永,曹明盛.中南矿冶学院学报,1981;(3) :1 3 Dunne D P, Kennon N F. Scr Metall, 1982; 16: 729 4 孔祥炎,高安娟.中南矿冶学院学报,1983;(2) :49 |
|