| WC-Co合金微裂纹形核过程的探讨 |
| 宋士泓;李健纯 |
| 中南工业大学;中南工业大学 |
|
| INITIATION OF MICROCRACKS IN WC-Co ALLOYS |
| by SONG Shihong; LI Jianchun (Central-South University of Technology) (Manuscript received 10 December 1985; revised manuscript 14 June; 1986) |
引用本文:
宋士泓;李健纯. WC-Co合金微裂纹形核过程的探讨[J]. 金属学报, 1987, 23(6): 521-526.
,
.
INITIATION OF MICROCRACKS IN WC-Co ALLOYS[J]. Acta Metall Sin, 1987, 23(6): 521-526.
1 Suzuki H, Hayashi K. Trans Jpn Inst Met, 1975; 16: 353 2 Suzuki H, Tanase T. Planseeber Pulvermetall, 1976; 242: 71 3 Roebuck B, Almond E A. Recent Advances in Hardmetal Production(Proc. Conf.), Loughborough University of rech. and Metall Powder Report, Vol. 2, 1979: 28 4 Chermant J L, Osterstock F. J Mater Sci, 1976; 11: 1939 5 Engel U, Huebner H. J Mater Sci. 1978; 13: 2003 6 Johannesson T, Lehtinen B, Philos Mag, 1971; 24: 1079 7 Hagege S, Nouet G, Delavignette P. Phys Status Solidi(a), 1980; 61: 675 8 Chermant J L, Deschanvres A, Osterstock F. Powder Metall, 1977; 2: 63 9 Gurland J. Jernkontorets Ann, 1963; 4: 147 10 宋士泓,刘武,李健纯.理化检验,物理分册,1987;23(1) :28 11 Jayaram V, Sinclair R, Rowcliffe D J. Acta Metall, 1983; 31: 373 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|